MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celcon® GC25A POM, 25% Glass Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Celcon« acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower mold shrinkage, minimum thermal expansion, excellent dimensional stability and good moldability.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccASTM D792
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
 0.0040 cm/cm0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/inISO 294-4
 0.014 cm/cm0.014 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 106 MPa15400 psi5mm/min; ISO 527-2/1A
 110 MPa16000 psiASTM D638
 68.9 MPa
@Temperature 71.1 °C
10000 psi
@Temperature 160 °F
ASTM D638
 159 MPa
@Temperature -40.0 °C
23000 psi
@Temperature -40.0 °F
ASTM D638
Elongation at Break 2.0 %2.0 %5mm/min; ISO 527-2/1A
Tensile Modulus 8.60 GPa1250 ksi50mm/min; ISO 527-2/1A
Flexural Strength 160 MPa23200 psiISO 178
Flexural Modulus 7.58 GPa1100 ksiASTM D790
 8.70 GPa1260 ksiISO 178
 3.45 GPa
@Temperature 104 °C
500 ksi
@Temperature 220 °F
ASTM D790
 4.83 GPa
@Temperature 71.1 °C
700 ksi
@Temperature 160 °F
ASTM D790
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inASTM D256
 0.374 J/cm
@Temperature -40.0 °C
0.700 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.481 J/cm
@Temperature 82.2 °C
0.900 ft-lb/in
@Temperature 180 °F
ASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179/1eU
 3.50 J/cm²
@Temperature -30.0 °C
16.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.640 J/cm²3.05 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.36e+14 ohm-cm1.36e+14 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C66.7 µin/in-°FISO 11359-2
Melting Point 165 °C329 °F10°C/min; ISO 11357-1,-2,-3
 166 °C331 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1, -2
 163 °C325 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 90.0 - 120 °C194 - 248 °Fcavity
 180 - 200 °C356 - 392 °Fhot runner
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 190 - 200 °C374 - 392 °F
Die Temperature 190 - 200 °C374 - 392 °F
Melt Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 90.0 - 140 MPa13100 - 20300 psi
Hold Pressure 90.0 - 140 MPa13100 - 20300 psi
Back Pressure <= 2.00 MPa<= 290 psi
 
Descriptive Properties
Injection moldingYes
Injection speedslow
PelletsYes
Processing conditions acc. ISO9988-2
Profile extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celcon® M90™ POM, Unfilled
Celanese Minlon® 10B40 NC010 PA66-MD40
Delrin Delrin® 100 BK602 POM
Overview of materials for Nylon 66, 20% Glass Fiber Filled
Celanese Celcon® GC25T POM, 25% Glass Reinforced

PHCQ103 / 178558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.