MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Iran Petrochemical (PCC) LS0085 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: LS0085 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.

Application: thin shrink film.

Information provided by Iran Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.921 g/cc0.0333 lb/in³ISO 1183
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.85 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.0 MPa1600 psiISO 527
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiISO 527
Elongation at Break 200 %200 %ISO 527, MD
 500 %500 %ISO 527, TD
Modulus of Elasticity 0.170 GPa24.7 ksiTD; ISO 527
 0.170 GPa24.7 ksiMD; ISO 527
Tensile Impact 250 J/cm468 ft-lb/inASTM D4272
Coefficient of Friction 1.01.0ASTM D1894
Tear Strength 30.0 kN/m171 pliTD; ISO 6383-2
 40.0 kN/m228 pliMD; ISO 6383-2
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003A
Gloss 55 %55 %ASTM D2457
 
Descriptive Properties
Clarity, mV30Sabtec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) MF3820 High Density Polyethylene
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene
Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene
Iran Petrochemical (PCC) LL22501 Linear Low Density Polyethylene
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene

PIPC249 / 149711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.