MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS BLACK PPE/Nylon Alloy 30% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled

Material Notes:

Information provided by PTS LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 138 MPa20000 psiASTM D638
Elongation at Break 7.5 %7.5 %ASTM D638
Flexural Strength 228 MPa33100 psiASTM D792
Flexural Modulus 7.58 GPa1100 ksiASTM D792
Izod Impact, Notched 0.908 J/cm
@Thickness 3.17 mm
1.70 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 246.1 °C475.0 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS PPE/Nylon Alloy 10% Glass Filled
Overview of materials for Nylon 63, 35% Glass-Filled
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry)
Celanese Celstran® PEHD-GF40-01 PE-HD, 40% Glass Reinforced
LATI Latene® HD 2 G/20 20% Glass Fiber Reinforced High Density Polyethylene (HDPE)

PZ9PU938 / 135395

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.