MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A27 E 01 PA66 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation "X Polyamide", 1.6.1998 or legislations for other countries will be provided on request.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³dry; ISO 1183
Water Absorption 8.5 %8.5 %beginning dry; ISO 62
Moisture Absorption at Equilibrium 2.2 %2.2 %beginning dry (23°C/50% R.H.); ISO 62
Viscosity Number 150 cm³/g1.50 dl/g
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM Data; MD
Melt Flow 80 g/10 min
@Load 5.00 kg,
Temperature 275 °C
80 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ISO 527
Elongation at Break >= 50 %>= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 20 %20 %50mm/min; ISO 527
Tensile Modulus 1.60 GPa232 ksi1mm/min; ISO 527
Flexural Modulus 7.60 GPa1100 ksiISO Data
Izod Impact, Notched (ISO) 9.50 kJ/m²4.52 ft-lb/in²ISO Test
Tensile Creep Modulus, 1 hour 1100 MPa160000 psiISO 899
Tensile Creep Modulus, 1000 hours 680 MPa98600 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+10 ohm-cm1.00e+10 ohm-cmIEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
5.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.20
@Frequency 1e+6 Hz
0.20
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10 K/min
 260 °C500 °FASTM Test
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21 CFR 177.1500
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
Impact ModifiedNo
Primary Processing TechniqueFilm Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A27 E 01 PA66 (Dry)
BASF Ultramid® A3K PA66 (Conditioned)
BASF Ultramid® A34 01 PA66 (Conditioned)
DuPont Mobility and Materials Zytel® FG101 NC010 PA66
BASF Ultradur® B 4520 BK00110 PBT

PBASF9210 / 84974

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.