MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9380A Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; very good hydrolysis and microbial resistance; good low-temperature flexibility; complies with VDE 0282-10; This product is manufactured under Good Manufacturing Practice (GMP defined in Regulation (EC) No. 2023/2006) and is therefore limited suitability for use with food contact. Application; Cable sheathings; Hoses, non-reinforced.

Mechanical property data for samples at 50% RH.

Information provided by Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 80
@Time 1.00 sec
80
@Time 0.000278 hour
DIN ISO 7619-1
Hardness, Shore D 31
@Time 1.00 sec
31
@Time 0.000278 hour
DIN ISO 7619-1
Tensile Strength, Ultimate 39.9 MPa5790 psi200mm/min; DIN 53504
Elongation at Break 594 %594 %200mm/min; DIN 53504
Tensile Modulus  0.0300 GPa
@Temperature 60.0 °C
4.35 ksi
@Temperature 140 °F
Tensile Storage Modulus; ISO 6721-1,-4
 0.0370 GPa
@Temperature 20.0 °C
5.37 ksi
@Temperature 68.0 °F
Tensile Storage Modulus; ISO 6721-1,-4
 0.0730 GPa
@Temperature -20.0 °C
10.6 ksi
@Temperature -4.00 °F
Tensile Storage Modulus; ISO 6721-1,-4
50% Modulus 3.90 MPa
@Strain 50 %
3.90 MPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus 5.20 MPa
@Strain 100 %
754 psi
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 9.40 MPa
@Strain 200 %
1360 psi
@Strain 200 %
200 mm/min; DIN 53504
Rebound 50 %50 %ISO 4662
Tear Strength 50.0 kN/m285 pli500mm/min; ISO 34-1
Abrasion 2020mm3; ISO 4649 method A, 50% RH
Compression Set  25 %
@Temperature 72.0 °C,
Time 82800 sec
25 %
@Temperature 162 °F,
Time 23.0 hour
DIN ISO 815-1
 25 %
@Temperature 70.0 °C,
Time 86400 sec
25 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method C
 37 %
@Temperature 70.0 °C,
Time 86400 sec
37 %
@Temperature 158 °F,
Time 24.0 hour
DIN ISO 815-1, Method A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 215 °C383 - 419 °Fextrusion
 205 - 225 °C401 - 437 °Finjection molding
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °Finjection molding
Drying Temperature <= 80.0 °C<= 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 3070AU Thermoplastic Polyurethane
Covestro Desmopan® 89043D Thermoplastic Polyurethane
Covestro Desmopan® 9370A Thermoplastic Polyurethane
Covestro Desmopan® 2590A Thermoplastic Polyurethane
Covestro Desmopan® 3385A Polyurethane

PB095013 / 200084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.