MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TEGO® Antifoam PVC 100 Organomodified siloxane
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam PVC 100 is an antifoam based on organomodified siloxane.

Application: TEGO® Antifoam PVC 100 destroys foam or so called “dry foam” reliably in formulations produced with dispersing agents like cellulose or polyvinyl alcohols:

  • Suspension-PVC
  • Ethylene-Vinyl-Acetate-Copolymers (EVAc)
  • Polyvinyl acetate (PVAc)
Properties / Benefits: TEGO® Antifoam PVC 100 might be used in all steps for the production of dispersions like reaction, blow down and stripping. TEGO® Antifoam PVC 100 outperforms conventional antifoams in several respects:
  • TEGO® Antifoam PVC 100 is high efficient in fighting dry foam where conventional anti-foams often fail.
  • TEGO® Antifoam PVC 100 shows an outstanding dispersibility and dilution stability.
  • undesirable effects associated with other organic or silicone antifoams are reduced or even eliminated.
  • Beside the antifoaming performance, TEGO® Antifoam PVC 100 improves the dewatering of S-PVC after stripping.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.02 g/cc0.0361 - 0.0368 lb/in³
Viscosity 160 - 230 cP160 - 230 cPdynamic
 
Descriptive Properties
Appearanceclear liquid
Content100%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TEGO® Antifoam 2280 Emulsion
BASF Glacial Acrylic Acid
BYK Laponite® JS Clay Additive
Solvay RHODAFAC® RE-610 E Surfactant
Henkel Turco Nova EC-202L Etchant

PEVONIL558 / 196762

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.