MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum 2124-T351
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
A Zr + Ti limit of 0.20 percent maximum may be used with this alloy designation for extruded and forged products only, but only when the supplier and the purchaser have mutually agreed.
Composition information provided by the Aluminum Association and is not for design.

Key Words: Aluminium 2124-T351; UNS A92124; QQ-A-250/29; ASTM B209; AMS 4101; AA2124-T351; Al2124-T351
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.78 g/cc0.100 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120120500 kg load with 10 mm ball
Hardness, Knoop 150150Converted from Brinell Hardness Value
Hardness, Rockwell A 4747Converted from Brinell Hardness Value
Hardness, Rockwell B 7575Converted from Brinell Hardness Value
Hardness, Vickers 137137Converted from Brinell Hardness Value
Tensile Strength, Ultimate 470 MPa68200 psi
Tensile Strength, Yield 325 MPa47100 psi
Elongation at Break 20 %20 %In 5 cm; Sample 1.6 mm thick
Modulus of Elasticity 73.0 GPa10600 ksiAverage of Tension and Compression. In Al alloys, the compressive modulus is typically 2% greater than the tensile modulus
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Fatigue Strength 140 MPa
@# of Cycles 5.00e+8
20300 psi
@# of Cycles 5.00e+8
Shear Modulus 27.0 GPa3920 ksiEstimated from similar Al alloys.
Shear Strength 285 MPa41300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000440 ohm-cm0.00000440 ohm-cmEstimated from other heat treatments.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.1 µm/m-°C
@Temperature -50.0 - 20.0 °C
11.7 µin/in-°F
@Temperature -58.0 - 68.0 °F
 22.9 µm/m-°C
@Temperature 20.0 - 100 °C
12.7 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 23.8 µm/m-°C
@Temperature 20.0 - 200 °C
13.2 µin/in-°F
@Temperature 68.0 - 392 °F
 24.7 µm/m-°C
@Temperature 20.0 - 300 °C
13.7 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.882 J/g-°C0.211 BTU/lb-°F
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°F
Melting Point 502 - 638 °C935 - 1180 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting is not eliminated by homogenization.
Solidus 502 °C935 °FAA; Typical
Liquidus 638 °C1180 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 493 °C920 °F
Aging Temperature 191 °C375 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 91.2 - 94.7 %91.2 - 94.7 %As remainder
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 3.8 - 4.9 %3.8 - 4.9 %
Iron, Fe <= 0.30 %<= 0.30 %
Magnesium, Mg 1.2 - 1.8 %1.2 - 1.8 %
Manganese, Mn 0.30 - 0.90 %0.30 - 0.90 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.20 %<= 0.20 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.25 %<= 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2124-T851 (Extended High Temperature Data)
Aluminum 2124-O
Aluminum 2124-T851
Aluminum 7075-T6; 7075-T651
Aluminum 5454-H34

MA2124T351 / 8914

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.