MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: 12 wt% Vinyl Acetate.

Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

Applications: Elvax® 3135X is designed to provide a low-temperature heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on blown film equipment over a wide range of film thicknesses and blow-up ratios. It can also be coextruded with a variety of other polymers. Films from this resin exhibit good puncture resistance, superior optics, a high degree of stretch, and are often used in stretch wrap and/or stretch bundling applications. Elvax® 3135X is also available in a specially formulated compound (Elvax® 3135AC) for those applications requiring added cling.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
Moisture Vapor Transmission 0.910 cc-mm/m²-24hr-atm
@Thickness 0.0254 mm
2.31 cc-mil/100 in²-24hr-atm
@Thickness 0.00100 in
g-mm/m²-day; based on film thickness; ASTM E96; ASTM E96
Oxygen Transmission 201 cc-mm/m²-24hr-atm
@Thickness 0.0254 mm
511 cc-mil/100 in²-24hr-atm
@Thickness 0.00100 in
film; ASTM D3985
Viscosity 2.00e+6 cP
@Shear Rate 50 1/s,
Temperature 190 °C
2.00e+6 cP
@Shear Rate 50 1/s,
Temperature 374 °F
estimated from log-log graph
Melt Flow 0.35 g/10 min0.35 g/10 minCondition not noted.; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 550 %550 %50 µm (2 mil) film; ASTM D882
Film Elongation at Break, TD 550 %550 %50 µm (2 mil) film; ASTM D882
Secant Modulus, MD 0.0580 GPa8.41 ksi50 µm (2 mil) film; ASTM D882
Secant Modulus, TD 0.0650 GPa9.43 ksi50 µm (2 mil) film; ASTM D882
Impact 43.643.6J/mm Spencer Impact; Average of MD and TD; ASTM D3420
Coefficient of Friction 1.31.3film/metal; ASTM D1894
 3.43.4film/film; ASTM D1894
Elmendorf Tear Strength, MD 3.19 g/micron81.0 g/mil50 µm (2 mil) film; ASTM D1922
Elmendorf Tear Strength, TD 3.35 g/micron85.0 g/mil50 µm (2 mil) film; ASTM D1922
Film Tensile Strength at Break, MD 32.0 MPa4640 psi50 µm (2 mil) film; ASTM D882
Film Tensile Strength at Break, TD 34.0 MPa4930 psi50 µm (2 mil) film; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 78.0 °C172 °FFreezing Point via DSC/ASTM D3418
 95.0 °C203 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 82.0 °C180 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %3.0 %ASTM D1003
Gloss 123 %123 %20°; ASTM D2457
Transmission, Visible 69 %69 %50 µm (2 mil) film; ASTM D1746
 
Processing PropertiesMetricEnglishComments
Melt Temperature 175 - 205 °C347 - 401 °Fblown film extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 3120 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
Dow Elvax® 3130 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
Dow Elvax® 3135SB Ethylene-Vinyl Acetate Copolymer Resin for Blown Film
Dow Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
Dow Elvax® 760 Ethylene Vinyl Acetate

PDUPH9 / 33612

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.