MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-ABS 2925 FR Flame Retardant ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: Data provided by Multibase.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ASTM D792-91
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238-94a
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 35.2 MPa5110 psiASTM D638-95
Elongation at Break 30 %30 %ASTM D638-95
Flexural Modulus 2.00 GPa290 ksiRT; ASTM D-790-95
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 35.4 kV/mm899 kV/inASTM D149-95
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 161 °C322 °Finjection molded unannealed; ASTM D-648-95
 195 °C383 °Fcompression molded annealed; ASTM D-648-95
 196 °C385 °Finjection molded annealed; ASTM D-648-95
Vicat Softening Point 99.0 °C210 °FASTM D1525-95
Flammability, UL94  V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
5V
 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Daicel CEVIAN® SER91 ABS
Cossa Polimeri ESTADIENE 1218 HT V0 Flame Retardant ABS
Cossa Polimeri ESTADIENE 1030 V0/Ex Flame Retardant ABS
Cossa Polimeri ESTADIENE 1030 T V0 Flame Retardant ABS
Cossa Polimeri ESTADIENE 1030 HT V0 Flame Retardant ABS

PLA289 / 49686

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.