MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SIDPEC EGYPTENE® LL 2406 AA LLDPE Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Applications:
  • Drip irrigation pipe
  • Small potable water pipe

Information provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.924 g/cc0.0334 lb/in³ISO 1872/1
ESCR, Bottle 250 hour
@Temperature 50.0 °C
250 hour
@Temperature 122 °F
BP 13C/25
Melt Flow 0.65 g/10 min
@Load 2.16 kg
0.65 g/10 min
@Load 4.76 lb
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 11.8 MPa1710 psiBP 13B/1
Elongation at Break 1000 %1000 %BP 13B/1
Flexural Modulus 0.400 GPa58.0 ksiISO 178-1975

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem LL6800N LLDPE Blown Film Extrusion Polyethylene Copolymer
NOVA Chemicals Novapol® PP-0118-F LLDPE Extrusion Resin
LyondellBasell Petrothene® GA818073 Linear Low Density Polyethylene
Ipiranga Petrochem LB 0117 LLDP
APCM DA 2406 Two Part Epoxy Adhesive Fast Set

PSIDP20 / 67715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.