MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik TROGAMID® CareMX97 Polyamide
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: TROGAMID® Care grades represent a range of both amorphous and microcrystalline transparent polyamides for processing via extrusion or injection molding. Durable: Microcrystalline TROGAMID® Care MX is the material of choice for all applications dealing with pharmaceutical formulations, lipids or aggressive disinfectants, since it exhibits an exceptional resistance towards chemicals and stress-cracking. Examples include fluid and drug delivery equipment such as stop-cocks, dialyzer parts, housings, covers or hearing aids. The high mechanical stability of amorphous TROGAMID® Care MT50 predestines the material for applications requiring a high modulus but retaining impact resistance which includes e.g. dentures, parts for monitoring and imaging devices or durable medical equipment. It comprises one of the highest tensile moduli compared to other transparent polyamides. Functional The antibacterial TROGAMID® Care MX73-A was designed to protect medical devices from surface bacterial colonization, while preserving its outstanding resistance to chemicals and stress-cracking as well as transparency. ISO 22196 tests conducted with E. coli and S. aureus showed a reduction of the viable cell count of more than 99.99%, each. TROGAMID® Care MX73-L is a transparent specialty grade for applications involving laser welding and laser marking. Though appearing transparent and colorless, it absorbs laser radiation, wherefore the combination of TROGAMID® Care MX73 and MX73-L enables the connection of two transparent parts via laser-welding, omitting exposure of the materials to extensive heat treatments or usage of adhesives. Target areas of application for TROGAMID® Care MX compounds include fluid and drug delivery systems, surgical instruments, housings, monitoring and imaging devices and durable medical equipment.

All advantages at a glance

  • High transparency
  • High chemical resistance
  • Very good stress crack resistance
  • UV resistance
  • High dynamic load-bearing capacity
  • Easy processability & colorability
  • Free of BPA

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³ISO 1183
Water Absorption at Saturation 3.5 %3.5 %ISO 62
Linear Mold Shrinkage, Flow 0.0065 cm/cm0.0065 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8181ISO 868
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-1
Elongation at Break >= 50 %>= 50 %ISO 527-1
Elongation at Yield 8.0 %8.0 %ISO 527-1
Tensile Modulus 1.40 GPa203 ksiISO 527-1/-2
Flexural Modulus 1.70 GPa247 ksiISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.30 J/cm²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359
Melting Point 250 °C482 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 122 °C252 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °FISO 75-1/-2
Vicat Softening Point  130 °C
@Load 5.10 kg
266 °F
@Load 11.2 lb
ISO 306
 135 °C
@Load 1.02 kg
275 °F
@Load 2.25 lb
ISO 306
Glass Transition Temp, Tg 140 °C284 °FISO 11357
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik TROGAMID® CareMX73 Polyamide
Evonik TROGAMID® CX9704 Polyamide
Evonik Trogamid® T5002 Nylon 6-3 Compound
Evonik TROGAMID® CareMT50 Polyamide
Evonik TROGAMID® CX7323 Polyamide

PEVONIL192 / 196396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.