MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® 4068FG TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D High Performance Polyester Elastomer Developed for Food Contact Applications

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 g/cc0.0401 lb/in³ISO 1183
Water Absorption 0.70 %
@Thickness 2.00 mm
0.70 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.300 %
@Thickness 2.00 mm
0.300 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
Melt Flow  8.5 g/10 min
@Load 2.16 kg,
Temperature 220 °C
8.5 g/10 min
@Load 4.76 lb,
Temperature 428 °F
ISO 1133
 8.8 g/10 min
@Load 2.16 kg,
Temperature 220 °C
8.8 g/10 min
@Load 4.76 lb,
Temperature 428 °F
cm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 313115s; ISO 48-4
 <= 37<= 37ISO 48-4
Tensile Stress at Strain  2.40 MPa
@Strain 5.0 %
348 psi
@Strain 5.0 %
1BA specimen at 50mm/min; ISO 527-1/-2
 3.50 MPa
@Strain 10 %
508 psi
@Strain 10 %
ISO 527-1/-2
 6.70 MPa
@Strain 50 %
972 psi
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 0.0470 GPa6.82 ksiISO 178
Izod Impact, Notched (ISO)  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 180/1A
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
Tensile Impact Strength 145 kJ/m²
@Temperature 23.0 °C
69.0 ft-lb/in²
@Temperature 73.4 °F
Notched; ISO 8256/1
Tear Strength 100 kN/m571 pliparallel; ISO 34-1
 103 kN/m588 plinormal; ISO 34-1
Abrasion 180180mm3; ISO 4649
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.8
@Frequency 100 Hz
4.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 230 µm/m-°C128 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 230 µm/m-°C128 µin/in-°FISO 11359-1/-2
Melting Point 193 °C379 °F10°C/min; ISO 11357-1/-3
Glass Transition Temp, Tg -50.0 °C-58.0 °F10°C/min; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 215 °C419 °FOptimum, Extrusion
 210 - 225 °C410 - 437 °FRange, Extrusion
 225 °C437 °FOptimum, Injection
 220 - 250 °C428 - 482 °FRange, Injection
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °FInjection
 40.0 °C104 °FOptimum, Injection
Drying Temperature 100 °C212 °FInjection
 90.0 - 110 °C194 - 230 °FExtrusion
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hour2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Eff. thermal diffusivity (m²/s)5.44E-08
Emission of organic compounds (µgC/g)10VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Odor Class4VDA 270
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® 4069 TPC-ET
Envalior Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America)
Celanese Hytrel® 4068 TPC-ET
Celanese Hytrel® 4056 TPC-ET
Celanese Hytrel® 4556 TPC-ET

PDSX5177 / 197817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.