MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Premi-Glas® 1200H-30 Fiberglass Reinforced Thermoset SMC
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset

Material Notes: Premi-Glas® 1200H-30 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.

Key features and benefits are:

  • Good dimensional stability, including excellent thermal resistance
  • Pigmentable for molded-in color; best appearance with mold texture
  • Excellent property retention in cold and hot environments
  • Suitable for outdoor use in applications involving UV exposure and water immersion in accordance with UL746C (f1), see file E42524
  • Designed for compression molding in matched metal die molds.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 - 1.85 g/cc1.70 - 1.85 g/cc
Linear Mold Shrinkage 0.0015 - 0.0025 cm/cm0.0015 - 0.0025 in/inPolymerization Shrinkage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 75.0 MPa10900 psiASTM D638
Tensile Modulus 12.0 GPa1740 ksiASTM D638
Flexural Strength 180 MPa26100 psiASTM D790
Flexural Modulus 11.0 GPa1600 ksiASTM D790
Compressive Strength 215 MPa31200 psiASTM D695
Poissons Ratio 0.300.30
Shear Modulus 4.60 GPa667 ksiCalculated
Izod Impact, Notched 8.00 J/cm15.0 ft-lb/inASTM D256
Izod Impact, Unnotched 11.5 J/cm21.5 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 15.0 kV/mm381 kV/inASTM D149
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C19.4 µin/in-°FZ Direction
CTE, linear, Transverse to Flow 25.0 µm/m-°C13.9 µin/in-°FXY Direction
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°F
UL RTI, Electrical 130 °C266 °FUL 746C
UL RTI, Mechanical with Impact 130 °C266 °FUL 746C
UL RTI, Mechanical without Impact 130 °C266 °FUL 746C
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 °C302 °FCompression Molding
Clamp Pressure 3.45 - 6.89 MPa500 - 1000 psiMolding Pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC
A. Schulman Premi-Glas® 1200H-10 Fiberglass Reinforced Thermoset SMC
C-Glass Fiber, Generic
A. Schulman Premi-Glas® 1200-30 Polyester SMC

PPREMH956 / 140354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.