MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Europrene® SOL TH 2315 Styrene - Ethylene / Butylene Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Europrene® SOL TH 2315 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where bound styrene content is 32%wt. A non-staining, TNPP free antioxidant system is added during the production process.

Key Features: Europrene® SOL TH 2315 is a linear triblock copolymer of high molecular weight, specifically designed to be formulated with high contents of processing oils and mineral fillers. The grade is characterized by excellent mechanical properties and ageing resistance.

Main Applications: Europrene® SOL TH 2315 is designed for technical compound applications. High performance compounds base on Europrene® SOL TH 2315 show excellent elastic and tensile characteristics, in a wide range of flowability and hardness.

Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow <= 1.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6868ASTM D2240
Tensile Strength at Break 25.0 MPa3630 psiASTM D412
Elongation at Break 600 %600 %ASTM D412
300% Modulus 3.50 MPa
@Strain 300 %
508 psi
@Strain 300 %
ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis Europrene® SOL TH 2314 Styrene - Ethylene / Butylene Block Copolymer
Versalis Europrene® SOL TH 2312 Styrene - Ethylene / Butylene Block Copolymer
Versalis Europrene® SOL TH 2311 Styrene - Ethylene / Butylene Block Copolymer
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Dynasol Solprene® 412 Thermoplastic Elastomer

PENG221 / 124615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.