MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Flint Hills AP5206-HN Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Features: Nucleated for fast cycle and good mold release. Product does not contain animal derived components.

Applications: Compression and injection molding: caps and closures

Information Provided by Flint Hills Resources

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 104104ASTM D785
Tensile Strength, Yield 30.3 MPa4390 psiASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus, 1% Secant 1517 MPa220000 psiASTM D790
Izod Impact, Notched 1.07 J/cm
@Temperature 23.0 °C
2.00 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Gardner Impact 9.00 J
@Temperature -30.0 °C
6.64 ft-lb
@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1586 MPa230000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C226 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Maxxam™ FR PP 301 S Polypropylene
Celanese Celstran® PP-GF30-03 PP, 30% Glass Reinforced
Celanese Celstran® PP-GF30-03 Natural PP, 30% Glass Reinforced
Ineos H02C-00 Polypropylene Homopolymer
Flint Hills AP5995-HA Polypropylene Impact Copolymer

PFLINT014 / 104568

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.