MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Avient Therma-Tech™ NJC-6000 TC Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of thermoplastics. These materials provide the benefits of proprietary conductive additive technologies and the performance of select engineering thermoplastic resins. Therma-Tech compounds have been shown to improve thermal conductivity up to 100-times that of conventional plastics and can be used in a wide range of thermal management applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccASTM D792
Water Absorption 0.10 %
@Thickness 3.18 mm,
Time 86400 sec
0.10 %
@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 49.0 MPa7110 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 0.90 %0.90 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 19.3 GPa2800 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
Flexural Modulus 19.4 GPa2810 ksiASTM D790
Izod Impact, Notched 0.267 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.500 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 - 1000 ohm-cm100 - 1000 ohm-cmASTM D257
Surface Resistance 10 - 100 ohm10 - 100 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 11.0 W/m-K76.3 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 193 °C
@Thickness 6.35 mm
379 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
@Thickness 6.35 mm
365 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 277 °C500 - 531 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
 
Descriptive Properties
FeaturesElectrically Conductive
 Thermally Conductive
FormsPellets
Generic NamePolyamide 12 (Nylon 12)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Automotive Under the Hood
 Consumer Applications
 Electrical/Electronic Applications
 Housings
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Therma-Tech™ NNC-5000 TC Polyamide 66 (Nylon 66)
Avient Therma-Tech™ NJ-6000 TC Polyamide 12 (Nylon 12)
Avient Therma-Tech™ NJC-7500 TC Nylon 12
Envalior Stanyl® TC502 PA46
RTP Company RTP 200 TC-C-40 FR Nylon 6/6 (PA), Thermally Conductive - Electrically Conductive - Flame Retardant

PH1PN9506 / 103342

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.