MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties allow engineers and designers the ability to create cost-effective, innovative parts that exhibit outstanding wear, heat, electrical and chemical resistance. The TECAPEEK™ family is made up of materials for medical applications.

  • TECAPEEK™ MT, unfilled pigmented medical grade PEEK
  • TECAPEEK™ XP98, compression molded 30% carbon fiber filled PEEK (isotropic properties)
  • TECAPEEK™ MT CF30, extruded 30% carbon fiber filled PEEK
  • TECAPEEK™ Classic™, ISO 10993 certification by resin and extrusion lot of 30 days contact
  • TECAPEEK™ Classix™ XRO-20 radio opaque grade with 20% BaSO4 added

The TECAPEEK™ family of high performance plastics are high effective in the creation and manufacture of high quality medical instruments. Five separate grades, each with qualities to meet a wide range of requirements for the engineer and product designer.

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.41 g/cc1.41 g/ccASTM D792
Density 1.44 g/cc0.0520 lb/in³ASTM D792
Water Absorption at Saturation 0.060 %
@Temperature 22.8 °C,
Time 86400 sec
0.060 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 107107ASTM D785
Tensile Strength, Yield 186 MPa
@Temperature 22.8 °C
27000 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 1.1 %1.1 %ASTM D638
Tensile Modulus 12.999 GPa
@Temperature 22.8 °C
1885.4 ksi
@Temperature 73.0 °F
1% Secant; ASTM D638
Flexural Strength 318 MPa
@Temperature 22.8 °C
46100 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 12.8 GPa
@Temperature 22.8 °C
1850 ksi
@Temperature 73.0 °F
ASTM D790
Compressive Strength 240 MPa
@Temperature 22.8 °C
34800 psi
@Temperature 73.0 °F
ASTM D695
Shear Strength 97.2 MPa
@Temperature 22.8 °C
14100 psi
@Temperature 73.0 °F
Ultimate; ASTM D3846
Izod Impact, Notched 0.481 J/cm
@Temperature 22.8 °C
0.900 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.4 µm/m-°C8.00 µin/in-°FASTM D696
Thermal Conductivity 0.918 W/m-K6.37 BTU-in/hr-ft²-°FASTM C177
Melting Point 340 °C644 °F
Maximum Service Temperature, Air 260 °C500 °Fcontinuous
Deflection Temperature at 1.8 MPa (264 psi) 316 °C600 °FASTM D648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Limiting PV 2385000psi fpm, 68°F, 1200 in/min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber

PENSIN025 / 92842

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.