MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Film Grade

Material Notes: 4 wt% Methacrylic Acid.

Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits: Adhesion to metallized film. Excellent adhesion to PE. Better hot tack, sealability through contamination and heat seal strength compared to PE. Excellent optical properties.

Typical Applications: Tie layer in Surlyn®/TIE/PE type structures. Coextrusion with Nucrel® and PE in film structures. Thermal lamination to metal surfaces.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ASTM D792
Viscosity 1.10e+6 cP
@Shear Rate 50 1/s,
Temperature 190 °C
1.10e+6 cP
@Shear Rate 50 1/s,
Temperature 374 °F
estimated from log-log graph
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 596 %596 %50 µm (2 mil) film; ASTM D882
Film Elongation at Break, TD 628 %628 %50 µm (2 mil) film; ASTM D882
Secant Modulus, MD 0.162 GPa23.5 ksi50 µm (2 mil) film; ASTM D882
Secant Modulus, TD 0.171 GPa24.8 ksi50 µm (2 mil) film; ASTM D882
Impact 14.214.2J/mm Spencer Impact; ASTM D3420
Graves Tear Strength 69.9 kN/m399 pliMD; ASTM D1004
 78.8 kN/m450 pliTD; ASTM D1004
Elmendorf Tear Strength, MD 5.08 g/micron129 g/mil50 µm (2 mil) film; ASTM D1922
Elmendorf Tear Strength, TD 5.16 g/micron131 g/mil50 µm (2 mil) film; ASTM D1922
Dart Drop 3.90 g/micron99.1 g/milASTM D1709B
Seal Strength 2700 g/25 mm2700 g/inseal bar 150°C.
Hot Tack Strength 1400 g/25 mm1400 g/inseal bar 115°C; Packforsk method.
Film Tensile Strength at Break, MD 23.3 MPa3380 psi50 µm (2 mil) film; ASTM D882
Film Tensile Strength at Break, TD 24.8 MPa3600 psi50 µm (2 mil) film; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 92.0 °C198 °FFreezing Point via DSC/ASTM D3418
 104 °C219 °FUpon Melting via DSC/ASTM D3418
Vicat Softening Point 95.0 °C203 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 3.2 %3.2 %ASTM D1003
Gloss 82 %82 %20°; ASTM D2457
Transmission, Visible 56 %56 %50 µm (2 mil) film; ASTM D1746
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 210 °C410 °FTypical Die Temp.
Melt Temperature 190 - 218 °C374 - 424 °Fblown film equipment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
Dow Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film
Dow Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer

PDUPJ0 / 33634

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.