MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Ti-3Al-2.5V (Grade 9), Beta-Anneal 950°C
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Information provided by Allvac and the references. High strength-to-weight ratio, lighter than stainless steel. Good corrosion resistance in mildly reducing to highly oxidizing media.

Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems.

Forms typically available: Sheet, strip, foil and tubing.

3 other heat treatments of this alloy are in MatWeb.

Key Words: Ti3Al2.5V, UNS R56320; ASTM Grade 9; Half 6-4; Tubing Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.48 g/cc0.162 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 300300
Tensile Strength, Ultimate 620 MPa89900 psi
Tensile Strength, Yield 540 MPa78300 psi
Elongation at Break 17 %17 %
Modulus of Elasticity 100 GPa14500 ksiAlpha-annealed in tension.
Tensile Modulus 80.0 GPa
@Temperature 230 °C
11600 ksi
@Temperature 446 °F
Poissons Ratio 0.300.30alpha annealed
Fracture Toughness 70.0 MPa-m½63.7 ksi-in½kJ/m² for J(IC)
Shear Modulus 44.0 GPa6380 ksiAlpha-annealed
Charpy Impact 44.0 J32.5 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000127 ohm-cm0.000127 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.61 µm/m-°C
@Temperature 20.0 - 95.0 °C
5.34 µin/in-°F
@Temperature 68.0 - 203 °F
 9.67 µm/m-°C
@Temperature 20.0 - 205 °C
5.37 µin/in-°F
@Temperature 68.0 - 401 °F
 9.86 µm/m-°C
@Temperature 20.0 - 315 °C
5.48 µin/in-°F
@Temperature 68.0 - 599 °F
 9.97 µm/m-°C
@Temperature 20.0 - 540 °C
5.54 µin/in-°F
@Temperature 68.0 - 1000 °F
average
Specific Heat Capacity 0.525 J/g-°C0.125 BTU/lb-°FTypical value for titanium alloys.
Thermal Conductivity  11.8 W/m-K
@Temperature 23.0 °C
81.9 BTU-in/hr-ft²-°F
@Temperature 73.4 °F
 11.8 W/m-K
@Temperature 315 °C
81.9 BTU-in/hr-ft²-°F
@Temperature 599 °F
Melting Point <= 1700 °C<= 3090 °F
Solidus 1704 °C3099 °F
Liquidus 1700 °C3090 °F
Beta Transus 935 °C1720 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 2.5 - 3.5 %2.5 - 3.5 %
Carbon, C <= 0.050 %<= 0.050 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.030 %<= 0.030 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.30 %<= 0.30 %
Oxygen, O <= 0.15 %<= 0.15 %
Titanium, Ti 92.755 - 95.5 %92.755 - 95.5 %As Balance; Elemental Composition per ASTM B265
Vanadium, V 2.0 - 3.0 %2.0 - 3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Ti-3Al-2.5V (Grade 9), alpha annealed
Titanium Ti-3Al-2.5V (Grade 9), Alpha-Beta Anneal, Quenched
Titanium Ti-3Al-2.5V (Grade 9), ST 925°C, Aged 480°C (900°F)
Titanium Ti-6Al-4V (Grade 5), Annealed
Titanium Ti-5Al-2.5Sn (Grade 6)

MTA324 / 14126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.