MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

C.O.I.M. LARIPUR® LPR72D25 Special Adipate Ester Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyester Thermoplastic Elastomer; Polyurethane, TP

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 25 Special Adipate Ester: These products are based on saturated polyesters. Products are based on saturated polyester. The features are similar to those of Series 20 but, by comparison, they are characterized by a higher resistance to hydrolysis and improved flexibility at low temperatures.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6767ASTM D2240
Tensile Strength, Yield 72.2 MPa10500 psiASTM D412
Elongation at Break 320 %320 %ASTM D412
50% Modulus 25.3 MPa
@Strain 50 %
25.3 MPa
@Strain 50 %
ASTM D412
100% Modulus 27.7 MPa
@Strain 100 %
4020 psi
@Strain 100 %
ASTM D412
300% Modulus 30.3 MPa
@Strain 300 %
4390 psi
@Strain 300 %
ASTM D412
Flexural Modulus 0.530 GPa76.9 ksiASTM D790
Izod Impact, Notched (ISO) 3.50 kJ/m²
@Temperature -20.0 °C
1.67 ft-lb/in²
@Temperature -4.00 °F
ASTM D256
Tear Strength 228 kN/m1300 pliASTM D624
Abrasion 4040mm3, Abrasion Loss; DIN 53516
Torsional Stiffness 125 MPa18100 psi+20°C; ASTM D1043
 500 MPa72500 psi-20°C; ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 185 °C365 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR9025 Special Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5020 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR4525 Special Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5225 Special Adipate Ester Polyurethane

PCOIM014 / 28617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.