MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene™ FL 02020 Ethylene Vinyl Acetate Copolymer (European Grade)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product Description: FL 02020 is primarily designed for high speed/low coating weight extrusion coating and is a good coextrusion partner with other polymers. FL 02020 is an excellent sealing material with a very low seal initiation temperature, high clarity and low gel.
Processing Conditions: Excellent results are obtained in extrusion coating at 220°C (428°F) temperature range. Processing temperatures above 240°C (464°F) may cause resin degradation. FL 02020 should be fed into the extruder after LDPE of a similar or higher melt index. Machines should always be purged with LDPE or a suitable cleaning compound before shutdown.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Adhesive Lamination
  • Adhesive Layer onto OPP
  • Barrier Food Packaging
  • Cling Layer
  • Coextrusion Coating
  • Compounding
  • Document Plastification
  • Extrusion Coating
  • Extrusion Lamination
  • Flexible Packaging
  • High Frequency Sealing
  • Industrial Packaging
  • Injection Molding
  • Masterbatch Base Resin
  • Non-Woven Coating
  • PVC Replacement
  • Surface Protection Film
  • Thermal Lamination
  • Wire and Cable Compounds

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ExxonMobil method
Vinyl Acetate Content 20 %20 %ExxonMobil method
Melt Flow 20 g/10 min20 g/10 minASTM D1238
Neck In  8.89 cm
@Temperature 220 °C
3.50 in
@Temperature 428 °F
656 ft/min, constant output at 35 rpm; ExxonMobil Method
 10.7 cm
@Temperature 220 °C
4.20 in
@Temperature 428 °F
328 ft/min, constant output at 35 rpm; ExxonMobil Method
Drawdown 7.50 m/s
@Temperature 220 °C
1480 ft/min
@Temperature 428 °F
Constant output at 35 rpm; ExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 85
@Time 15.0 sec
85
@Time 0.00417 hour
Molded Properties; ISO 868
Tensile Strength at Break >= 0.689 MPa>= 100 psiMolded Properties; ISO 527-2/1A/100
Tensile Modulus 0.0262 GPa3.80 ksiMolded Properties; ISO 527-2/1
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 78.9 °C<= 174 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 48.3 °C119 °FASTM D1525
 
Descriptive Properties
Blending Temperature240

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil EVA 1718.CC3 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ FL 00714 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ UL 00119 Ethylene Vinyl Acetate Copolymer (European Grade)
ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade)

PEX99098 / 175334

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.