MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoplastic

Material Notes: AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, very low moisture absorption, is thermoformable and ductile. AIREX® R82 is a core material for use in structural lightweight applications that demand high fire resistance, radar transparency or operation in extremely hot or cold environments.

Characteristics

  • Fulfils most stringent fire requirements
  • Operating temperature from -194°C to +160°C (-317° F to +320 °F)
  • Remains ductile at cryogenic temperatures
  • Excellent dielectric properties (radar transparent outstanding)
  • Very low moisture absorption
  • Good fatigue resistance
  • High impact resistance (non-brittle failure mode)
  • Thermoformable
  • Good sound and thermal insulation
Applications
  • Aircraft and Aerospace: Interiors, cockpit doors, cryogenic tanks, insulating panels, radomes, helicopter rotor blades, general aviation (fuselage and wing)
  • Road and Rail: Front-ends, side skirts, roof panels, interiors
  • Marine: Fast-ferries, fire resistant interiors, radomes
  • Defense: Naval superstructures, antennas, combat communication systems
  • Industrial: High-temperature tooling, radomes, x-ray tables
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0600 g/cc0.00217 lb/in³average; ISO 845
 0.0540 - 0.0690 g/cc0.00195 - 0.00249 lb/in³typical range; ISO 845
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 1.20 MPa>= 174 psiin the plane; ISO 527 1-2
 1.70 MPa247 psiaverage; in the plane; ISO 527 1-2
Elongation at Break >= 15 %>= 15 %shear; ISO 1922
 25 %25 %average; shear; ISO 1922
Tensile Modulus >= 0.0350 GPa>= 5.08 ksiin the plane; ISO 527 1-2
 0.0450 GPa6.53 ksiaverage; in the plane; ISO 527 1-2
Compressive Strength >= 0.600 MPa>= 87.0 psiperpendicular to plane; ISO 844
 0.700 MPa102 psiaverage; perpendicular to plane; ISO 844
Compressive Modulus >= 0.0400 GPa>= 5.80 ksiperpendicular to plane; DIN 53421
 0.0460 GPa6.67 ksiaverage; perpendicular to plane; DIN 53421
Shear Modulus >= 0.0150 GPa>= 2.18 ksiASTM C393
 0.0180 GPa2.61 ksiaverage; ASTM C393
Shear Strength >= 0.650 MPa>= 94.3 psiISO 1922
 0.800 MPa116 psiaverage; ISO 1922
Charpy Impact, Notched 0.100 J/cm²0.476 ft-lb/in²DIN 53453
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0360 W/m-K0.250 BTU-in/hr-ft²-°FISO 8301
 
Descriptive Properties
Coloroff white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam
3A Composites Core Materials AIREX® C70.40 Universal Structural Foam
3A Composites Core Materials AIREX® C71.55 Elevated Temperature Structural Foam
3A Composites Core Materials AIREX® PXc.420 Fiber-Reinforced Structural Foam

PZ3AC025 / 108514

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.