MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

TriSteel

TriStar TriSteel AC Metal Backed PTFE Bearing System
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Ultraflon 601 (AC) POM lined metal backed bearing system, boundary lubrication required, high PV. Ultraflon 601 POM Liner is a lubricant enhanced acetal material for use in lubricated or unlubricated environments. With lubrication, PV ratings can be met without limitations. Lubrication reservoirs are available on the liner to produce a constant storage and pumping action for better hydrodynamic film generation.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Tensile Strength, Yield 51.7 MPa7500 psi
Elongation at Break 12 %12 %
Flexural Strength 103 MPa15000 psi
Flexural Modulus 1.03 GPa150 ksi
Compressive Strength 119 MPa17200 psi
 248 MPa36000 psiMaximum Static Bearing Load
Compressive Modulus 2.14 GPa310 ksi
Coefficient of Friction, Dynamic 0.190.19Dry vs Steel
K (wear) Factor 42.3 x 10-8 mm³/N-M21.0 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 2.80 MPa-m/sec80000 psi-ft/minUnlubricated. Max P = 36,000 psi and max V = 300 fpm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 4.32 W/m-K30.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C180 °FContinuous
 98.9 °C210 °FShort Term
Brittleness Temperature -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TriStar TriSteel AT Metal Backed PTFE Bearing System
TriStar TriSteel PE Metal Backed PTFE Bearing System
AISI 8620 Steel, quenched from carburizing box, 13 mm (0.5 in.) round
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Phosphorous, P, Red

PTRIST990 / 176084

TriSteel

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.