MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 1003-2 NF2002 PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 8.5 %8.5 %ISO 62
Moisture Absorption at Equilibrium 2.5 %2.5 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 83.0 MPa12000 psi2 in/min; ASTM Test
 85.0 MPa12300 psi50mm/min; ISO 527
Elongation at Break 25 %25 %50mm/min, Nominal strain; ISO 527
 60 %60 %2 in/min; ASTM Test
Elongation at Yield 5.0 %5.0 %50mm/min; ISO 527
Tensile Modulus 3.00 GPa435 ksi1mm/min; ISO 527
Flexural Strength 117 MPa17000 psiASTM Test
Flexural Modulus 2.80 GPa406 ksiISO Data
 2.90 GPa421 ksiASTM Test
Izod Impact, Notched 0.530 J/cm
@Thickness 3.17 mm
0.993 ft-lb/in
@Thickness 0.125 in
ASTM Test
Izod Impact, Notched (ISO) 5.20 kJ/m²2.47 ft-lb/in²ISO Test
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.570 J/cm²2.71 ft-lb/in²ISO 179
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 257 °C495 °F10 K/min
 257 °C495 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75
 243 °C469 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C162 °FISO 75
 88.0 °C190 °FASTM Test
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)
BASF Ultramid® 1310-11 NF2001 PA66 (Dry)
BASF Ultramid® 1000-2 NF2001 PA66 (Dry)
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned)
BASF Ultramid® A3K Q601 PA66(Dry)

PBASF9119 / 84883

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.