MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Heraeus Clevios™ F E Conductive Polymer
Categories: Polymer

Material Notes: Clevios™ F E is an aqueous dispersion of PEDOT:PSS conducting polymer that is formulated with polymeric binders and organic solvents. This high conductive ready-to-use formulation can be applied by conventional coating or printing techniques. Dried films exhibit bulk conductivity of 150 S/cm minimum.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³
Viscosity 10 - 30 cP10 - 30 cP
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 110 ohm110 ohm
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %
 
Processing PropertiesMetricEnglishComments
Cure Time 5.00 min0.0833 hour
 
Descriptive Properties
Conductive Filler TypeOrganic
Material TypeReady-To-Use Formulation
Recommended SubstratesDisplay Glass, PC, PET
Solvent Systemaqueous and organic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pau Tai UNISTAB PCZ-168 Non-toxic Calcium-Zinc Stabilizer
Gharda Chemicals Gafone™ T6300 Polysupersulfone (PSS)
Heraeus Clevios™ P Jet (OLED) Conductive Sulfonate Polymer for Antistatic Coatings
Heraeus Clevios™ F ET Conductive Polymer
Heraeus Clevios™ PH 1000 Conductive Sulfonate Polymer for Antistatic Coatings

PFLEXCM16 / 179418

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.