MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hanwha Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a very homogeneous fiber distribution. This material is typically used for standard semi-structural, thin wall applications.

Commercially available only to European based customers.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccLaminate; ISO 2577
 1.17 g/cc1.17 g/ccMolded plaque; ISO 2577
Filler Content 32 %32 %AZDEL Test
Thickness 4900 microns193 milAZDEL Test
Linear Mold Shrinkage 0.0028 cm/cm0.0028 in/in320 x 320 mm flat plaque; ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psiISO 527/4
Elongation at Break 2.6 %2.6 %ISO 527/4
Tensile Modulus 4.80 GPa696 ksiISO 527/4
Flexural Strength 135 MPa19600 psiISO 178
Flexural Modulus 4.40 GPa638 ksiISO 178
Charpy Impact, Notched 8.50 J/cm²40.5 ft-lb/in²ISO 179/2fn
Impact 5500
@Thickness 4.00 mm
5500
@Thickness 0.157 in
N; Multi-axial at max. force; ISO 6603-2
Impact Test  17.0 J
@Thickness 4.00 mm
12.5 ft-lb
@Thickness 0.157 in
Multi-axial, at max. force; ISO 6603-2
 45.0 J
@Thickness 4.00 mm
33.2 ft-lb
@Thickness 0.157 in
Multi-axial, total energy; ISO 6603-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear  36.0 µm/m-°C
@Temperature 0.000 - 120 °C
20.0 µin/in-°F
@Temperature 32.0 - 248 °F
100 x 15 x 3 mm sample; AZDEL Test
 48.0 µm/m-°C
@Temperature -30.0 - 0.000 °C
26.7 µin/in-°F
@Temperature -22.0 - 32.0 °F
100 x 15 x 3 mm sample; AZDEL Test
Melting Point 115 °C239 °FRecrystallizing temperature; ISO 3146
 166 °C331 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75/2a
 
Processing PropertiesMetricEnglishComments
Processing Temperature 205 - 220 °C401 - 428 °FSurface temperature
Mold Temperature 30.0 - 90.0 °C86.0 - 194 °F
Back Pressure 15.0 - 25.0 MPa2180 - 3630 psiDepending on wall thickness and part complexity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hanwha Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C321-B01 32% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix
Hanwha Azdel Plus C220-B01 22% Chopped Fiber Mat / PP Resin Matrix

PZZGEAZ75 / 40624

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.