MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Alumor 90 Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Tabular Alumina. Hydraulic bond. A 1800°C castable with very low iron content based on pure tabular alumina for use where extreme temperatures or chemical purity is needed.

Typical applications: Suitable for burner block applications in aluminium melting and holding furnaces.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 2.85 g/cc0.103 lb/in³dried to 110°C
Grain Size <= 6000 µm<= 6000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  40.0 MPa
@Treatment Temp. 815 °C
5800 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 40.0 MPa
@Treatment Temp. 1000 °C
5800 psi
@Treatment Temp. 1830 °F
Cold Crushing Strength
 50.0 MPa
@Treatment Temp. 110 °C
7250 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 70.0 MPa
@Treatment Temp. 1800 °C
10200 psi
@Treatment Temp. 3270 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.16 W/m-K
@Temperature 600 °C
15.0 BTU-in/hr-ft²-°F
@Temperature 1110 °F
Maximum Service Temperature, Air <= 1800 °C<= 3270 °F
Shrinkage  -0.500 - 0.50 %
@Treatment Temp. 1800 °C
-0.500 - 0.50 %
@Treatment Temp. 3270 °F
 0.00 - 0.20 %
@Treatment Temp. 110 °C
0.00 - 0.20 %
@Treatment Temp. 230 °F
 0.10 %
@Treatment Temp. 815 °C
0.10 %
@Treatment Temp. 1500 °F
 0.10 %
@Treatment Temp. 1000 °C
0.10 %
@Treatment Temp. 1830 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 97 %97 %
CaO 2.8 %2.8 %
Fe2O3 0.10 %0.10 %
K2O+Na2O 0.40 %0.40 %Na2O + K2O
MgO 0.10 %0.10 %
SiO2 0.10 %0.10 %
TiO2 0.10 %0.10 %
 
Descriptive Properties
Net Material Required (kg/m³)2790
Water Addition7-9% by weight, 1.75-2.25 L per bag, 25kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Kaolite 3300 High Temperature Insulating Castables
Thermal Ceramics Kaocast 3000 Dense Castable
Morgan Advanced Ceramics Kaolite 3300 Thermal Ceramic
Morgan Advanced Ceramics Kao-Tab® Monolithics 95 Thermal Ceramic

CMORF6320 / 203104

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.