MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

H.C. Starck Amperit® 335.066 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi)
Categories: Metal; Nonferrous Metal; Nickel Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Apparent Bulk Density 3.80 - 4.60 g/cc0.137 - 0.166 lb/in³ASTM B212
Particle Size 3.0 µm3.0 µmMaximum of 3% less than
 53 µm53 µmMaximum of 10% greater than
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6060
 
Component Elements PropertiesMetricEnglishComments
Boron, B 3.0 - 3.9 %3.0 - 3.9 %
Carbon, C 0.60 - 1.2 %0.60 - 1.2 %
Chromium, Cr 13 - 17 %13 - 17 %
Iron, Fe 3.0 - 6.0 %3.0 - 6.0 %
Nickel, Ni 68.4 - 77.1 %68.4 - 77.1 %
Silicon, Si 3.9 - 4.9 %3.9 - 4.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
H.C. Starck Amperit® 119.075 Molybdenum-Nickel SF RC 60 75-25 (Mo / NiSF)
H.C. Starck Amperit® 335.063 Nickel Self-fluxing Alloy HRC 60 (NiCrBSi)
AISI Type S2 Tool Steel, austenitized 845°C (1550°F), brine quenched to 15 HRC
Special Metals Nickel 200
AISI Type 651 (19-9) Stainless Steel cold rolled and stress relieved, 35 HRC hardness

NHCSTA056 / 17258

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.