MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MarkeTech Ceraflex 8Y Thin Zirconia Ceramic Oxygen Ion Conductor, Yttria Stabilized  (discontinued **)
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Data provided by the supplier, MarkeTech International.

8 mole% Y2O3 (13.8 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are both flexible and highly resilient. The high strength of CERAFLEX makes it easier to handle than other ceramic materials of the same thickness. CERAFLEX is available as strips, sheets, or custom parts. It is either partially or fully stabilized with yttria.

The fully stabilized material is an oxygen ion conductor and used to build solid oxide fuel cells and oxygen sensors. A new cesium stabilized material (CERAFLEX:Cs) with much better electrical conductivity is now available.

Properties and availability: Flatness 50 µm/in. Surface roughness 0.1 µm. Bending strength 40 kgf. Standard thicknesses 0.100 & 0.200 mm (up to 0.5 mm). Maximum size 200 x 200 mm.

MarkeTech International is no longer in business.

Key Words: ZrO2; Zirconium Oxides; YSZ
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.85 g/cc0.211 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  5.00 ohm-cm
@Temperature 1000 °C
5.00 ohm-cm
@Temperature 1830 °F
 10.0 ohm-cm
@Temperature 900 °C
10.0 ohm-cm
@Temperature 1650 °F
 20.0 ohm-cm
@Temperature 800 °C
20.0 ohm-cm
@Temperature 1470 °F
 30.0 ohm-cm
@Temperature 700 °C
30.0 ohm-cm
@Temperature 1290 °F
 120 ohm-cm
@Temperature 600 °C
120 ohm-cm
@Temperature 1110 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.50 µm/m-°C
@Temperature 20.0 °C
5.28 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 2.80 W/m-K19.4 BTU-in/hr-ft²-°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Yttrium-Stabilized Zirconia (YSZ) Single Crystal Substrate
American Elements Yttria stabilized Zirconia
Mateck YSZ
Solvay AB40N Breather fabric
Yttria Stabilized Zirconia, YSZ

C5MT41 / 362

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.