MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded; Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: PTFE G Standard Compound with glass fiber
Properties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).
Applications: Valve seats, seals, bearings, required to resist sliding and chemicals.

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.18 - 2.21 g/cc0.0788 - 0.0798 lb/in³extruded; ASTM D792
 2.19 - 2.22 g/cc0.0791 - 0.0802 lb/in³molded; ASTM D792
Deformation  6.0 - 7.0 %
@Pressure 13.7 MPa,
Time 86400 sec
6.0 - 7.0 %
@Pressure 1990 psi,
Time 24.0 hour
after 24hr relaxation; ASTM D621
 10 - 14 %
@Pressure 13.7 MPa,
Time 86400 sec
10 - 14 %
@Pressure 1990 psi,
Time 24.0 hour
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60 - 6560 - 65molded; ASTM D2240
 60 - 6560 - 65extruded; ASTM D2240
Tensile Strength >= 15.0 MPa>= 2180 psiextruded; ASTM D4894, ASTM D4745
 17.0 - 24.0 MPa2470 - 3480 psimolded; ASTM D4894, ASTM D4745
Elongation at Break >= 200 %>= 200 %extruded; ASTM D4745
 250 - 300 %250 - 300 %molded; ASTM D4894
Compressive Yield Strength 6.00 - 7.00 MPa
@Strain 1 %
870 - 1020 psi
@Strain 1 %
ASTM D695
Coefficient of Friction, Dynamic 0.120.12ASTM D1894
K (wear) Factor 10.0 - 20.0 x 10-8 mm³/N-M4.96 - 9.93 x 10-10 in³-min/ft-lb-hrat PV 100; ASTM D3702
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 - 130 µm/m-°C61.1 - 72.2 µin/in-°FASTM D696
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -200 °C-328 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
Polikim EFALON® C-15 PTFE, 15% Glass Filled
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide
Guarniflon PTFE G436 Polytetrafluoroethylene 3% Molybdenum Disulfide

PGUARN006 / 142739

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.