MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Montell SE191 Polypropylene Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: excellent electrical and physical properties, excellent resistance to environmental and thermal stress-cracking, low density an low dielectric constant contribute to light and smaller cables, tailored for high speed processing on thin-walled constructions

Applications: telephone singles general primary insulation

All ingredients meet TSCA (US) and DSL (Canada) registration requirements.

Description: Pro-fax SE191 low melt flow, electrical grade polypropylene copolymer resin has outstanding toughness, flex-life and abrasion resistance. This resin demonstrates good processing behavior and is tailored for trouble-free production of primary cable insulation, especially filled telephone cable because its unique stabilizer system resists extraction by petroleum-jelly based filling compounds. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792B
Environmental Stress Crack Resistance >= 200 hour>= 200 hourASTM D1693
Melt Flow 2.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.7 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.0 MPa3190 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus, 1% Secant 1000 MPa145000 psi0.05 in/min; ASTM D790A
Impact Test >= 60.0 J
@Temperature -29.0 °C
>= 44.3 ft-lb
@Temperature -20.2 °F
Montell drop weight impact strength
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmASTM D257
Dielectric Constant  2.25
@Frequency 100000 Hz
2.25
@Frequency 100000 Hz
 2.25
@Frequency 1e+6 Hz
2.25
@Frequency 1e+6 Hz
Dissipation Factor  0.00030
@Frequency 100000 Hz
0.00030
@Frequency 100000 Hz
ASTM D1531
 0.00030
@Frequency 1e+6 Hz
0.00030
@Frequency 1e+6 Hz
ASTM D1531
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHN-230 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHM-200 Polypropylene Impact Copolymer

PMO252 / 53573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.