MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

Westlake Plastics Kynar® 740 PVDF Homopolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: KYNAR polyvinylidene fluoride is a tough engineering thermoplastic that offers a unique balance of performance properties. It has the characteristic stability of fluoropolymers when exposed to harsh thermal, chemical and ultraviolet environments. KYNAR is also inherently UV stable, mechanically tough, abrasion and flame resistant. Resin meets the requirements of FDA, USDA, USP VI, Dairymen 3A, UL V-0, FM 4910

Applications include:

  • Semiconductor Packaging, Process and Testing Components
  • Semiconductor Wet Processing Components
  • Chemical Process/Storage tanks
  • Chemical tank liners
  • Fire Safety Components
  • DI Water System Components
  • Electrical Insulating Components
  • Radiation Barriers

Kynar® is a trademark of Arkema Group. Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.78 g/cc1.78 g/ccASTM D792
Water Absorption 0.030 %0.030 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 76 - 8076 - 80ASTM D2240
Tensile Strength, Yield 44.8 - 55.2 MPa6500 - 8000 psiASTM D638
Elongation at Break 20 - 100 %20 - 100 %ASTM D638
Elongation at Yield 7.0 - 13 %7.0 - 13 %ASTM D638
Tensile Modulus 1.38 - 2.31 GPa200 - 335 ksiASTM D638
Flexural Strength 58.6 - 75.8 MPa8500 - 11000 psiASTM D790
Flexural Modulus 1.38 - 2.31 GPa200 - 335 ksiASTM D790
Izod Impact, Notched 0.961 - 2.14 J/cm1.80 - 4.00 ft-lb/inASTM D256
Izod Impact, Unnotched 10.7 - 42.7 J/cm20.0 - 80.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+14 ohm-cm2.00e+14 ohm-cmASTM D257
Dielectric Constant 4.5 - 9.5
@Frequency 1000 Hz
4.5 - 9.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 63.0 kV/mm
@Thickness 0.127 mm
1600 kV/in
@Thickness 0.00500 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 µm/m-°C66.0 µin/in-°FASTM D696
Melting Point 165 - 172 °C329 - 342 °FASTM D4591
Maximum Service Temperature, Air 138 °C280 °FContinuous Use
Deflection Temperature at 0.46 MPa (66 psi) 125 - 140 °C257 - 284 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 - 115 °C221 - 239 °FASTM D648
Flammability, UL94 V-0V-0
Oxygen Index 75 %75 %ASTM D2868
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYes
FDA YesYes
USDA YesYes
USP Class VI YesYes
 
Descriptive Properties
ColorNatural Beige, Black, Red

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Omnia Plastica Kynar® PVDF
Westlake Plastics Kynar® 1000HD PVDF Homopolymer
GEHR Plastics PVC type I®
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded

PWEST140 / 72759

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.