MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Stanyl® TS272A1 PA46-RF, Aramid Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46)

Material Notes: Aramid fiber reinforced, Wear and Friction Modified

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Moisture Absorption 3.00 %3.00 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.022 cm/cm0.022 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psiISO 527-1/-2
Elongation at Break 20 %20 %ISO 527-1/-2
Tensile Modulus 2.80 GPa406 ksiISO 527-1/-2
Flexural Modulus 2.40 GPa348 ksiISO 178
Charpy Impact, Notched 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 72-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cathay PA510 Renewable Engineering Polyamide
Cathay Terryl® PA510 Renewable Engineering Polyamide Fiber
Envalior Stanyl® TE351 PA46 FR(17), Dry, Flame Retardant, Heat Stabilized
Envalior Stanyl® TE373 PA46, Dry, Heat Stabilized
Overview of materials for Nylon 66, Aramid Fiber Filled

PDSM8230 / 184931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.