MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex APEX® 130 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Notes: 80°C Jacket; RoHS Compliant

Features: Sunlight Resistant (720 hours); Good UV Resistance

Uses: Appliance Wire Jacketing; Building Wire Jacketing; Flexible Cord Jacketing; Wire and Cable Applications

Agency Ratings: UL QMTT2 .E73402

Forms: Pellets

Wire Types: AWM; SJTW; SRDT; STW; SVT; UF; UL Style 2835

Processing Method: Extrusion

Additional Information:

UL Recognized Component as PVC 300 Hour Sunlight Resistant Jacket Compound, QMTT2

UL Recognized as PVC 720 Hour Sunlight Resistant Insulation and Jacket Compounds, QMTT2

1/32 in wall

Temperature Rating: 80°C

UL Recognized Insulation: No

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 113°C: 89%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 113°C: 103%

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/ccASTM D792
Melt Flow 1.6 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.6 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 808010 seconds; ASTM D2240
Tensile Strength at Break 15.9 MPa2300 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FContinuous Use; ASTM D794
Brittleness Temperature -30.0 °C-22.0 °FASTM D746
Oxygen Index 22 %22 %ASTM D2863
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex APEX® 124 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 3201-55NT Polyvinyl Chloride, Flexible
Teknor Apex APEX® 3201-50NT Polyvinyl Chloride, Flexible
Teknor Apex APEX® 3200-90NT Polyvinyl Chloride, Flexible
Teknor Apex APEX® 3200-85 NT Polyvinyl Chloride, Flexible

PTEKNO480 / 128657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.