MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Escorene® LD 755.CM Molding, extrusion and compounding resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade

Material Notes: Escorene Ultra LD 755.CM is a high vinyl acetate copolymer for specialty compounding applications and hot melt adhesives.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Compounding
  • Hot Melt Adhesives
  • Master Base Resin

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ExxonMobil Method
Vinyl Acetate Content 27.6 %27.6 %ExxonMobil Method
Melt Flow 25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 707015s; ASTM D2240
Hardness, Shore D 191915s; ASTM D2240
Tensile Strength at Break 4.83 MPa700 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus, 1% Secant 18.6 MPa2700 psiASTM D790
Instrumented Impact Total Energy  14.9 J
@Temperature 23.0 °C
11.0 ft-lb
@Temperature 73.4 °F
ASTM D3763
 25.8 J
@Temperature -40.0 °C
19.0 ft-lb
@Temperature -40.0 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Melting Point 66.1 °C151 °FPeak Melting Temperature; ExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Escorene® LD-752 EVA Copolymer for Specialty Applications
Honeywell A-C® 715 PE homopolymer
RTP Company RTP 702 Z  High Density Polyethylene (HDPE) Glass Fiber 15% - FDA Type
Celanese Ateva® 1081G Medical Grade EVA
Bakelite® UP 804 Unsaturated Polyester Resin, High Surface Quality, UL Listed, Low Shrinkage, High Arc Resistance

PEXB152a / 140960

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.