MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (719°C)/8 h/FC at 100°F (56°C)/h to 1150°F (621°C) plus 1150°F (621°C)/8 h/AC. Heat capacity, melting range, moduli, and Poisson's ratio reported herein are typical of INCONEL® alloy 718SPF (not necessarily annealed + aged samples).

Data provided by the manufacturer, Special Metals.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.22 g/cc0.297 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 4545
Tensile Strength, Ultimate 1550 MPa225000 psi
Tensile Strength, Yield 1390 MPa
@Strain 0.2 %
202000 psi
@Strain 0.2 %
Elongation at Break 16 %16 %
Modulus of Elasticity 205 GPa29700 ksicold-rolled, heat treated sheet
Poissons Ratio 0.2940.294cold-rolled, heat treated sheet
Shear Modulus 80.0 GPa11600 ksicold-rolled, heat treated sheet
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000120 ohm-cm0.000120 ohm-cm
Magnetic Permeability 1.00111.0011at 200 Oersted (15.9 kA/m); Annealed
Curie Temperature -113 °C-171 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  12.15 µm/m-°C
@Temperature 21.0 - 93.0 °C
6.750 µin/in-°F
@Temperature 69.8 - 199 °F
Mean
 13.77 µm/m-°C
@Temperature 21.0 - 316 °C
7.650 µin/in-°F
@Temperature 69.8 - 601 °F
Mean
 14.4 µm/m-°C
@Temperature 21.0 - 538 °C
8.00 µin/in-°F
@Temperature 69.8 - 1000 °F
Mean
Specific Heat Capacity 0.435 J/g-°C0.104 BTU/lb-°F
Thermal Conductivity 11.4 W/m-K79.1 BTU-in/hr-ft²-°F
Melting Point 1260 - 1335 °C2300 - 2435 °F
Solidus 1260 °C2300 °F
Liquidus 1335 °C2435 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.20 - 0.80 %0.20 - 0.80 %
Boron, B <= 0.0060 %<= 0.0060 %
Carbon, C <= 0.050 %<= 0.050 %
Chromium, Cr 17 - 21 %17 - 21 %
Cobalt, Co <= 1.0 %<= 1.0 %
Copper, Cu <= 0.30 %<= 0.30 %
Iron, Fe 19 %19 %As remainder
Manganese, Mn <= 0.35 %<= 0.35 %
Molybdenum, Mo 2.8 - 3.3 %2.8 - 3.3 %
Nickel, Ni 50 - 55 %50 - 55 %Including Cobalt
Niobium, Nb (Columbium, Cb) 4.75 - 5.25 %4.75 - 5.25 %Includes Ta
Nitrogen, N <= 0.010 %<= 0.010 %
Phosphorus, P <= 0.015 %<= 0.015 %
Silicon, Si <= 0.35 %<= 0.35 %
Sulfur, S <= 0.0020 %<= 0.0020 %
Titanium, Ti 0.65 - 1.15 %0.65 - 1.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed
MetalTek MTEK 718 Cast UNS N07718 Severe Corrosion and Heat Resistant Alloy
Special Metals INCONEL® Alloy 718
Universal Wire Works Inconel 718 (AMS 5832) Filler Metal
Proto Labs Inconel 718 - DMLS

NINCO54 / 17487

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.