MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

CHT Group EP QS EPI Engineered Polymers Quick Set Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: EP QS Quick Set Epoxy, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, self-leveling modified epoxy. This versatile new generation epoxy displays low blush, fast cure times, and excellent adhesion characteristics. EP QS can be used as a surface tolerant primer or as a final coat, and will cure in a variety of harsh situations including high humidity. EP QS can be applied at temperatures ranging from 40° F to 120° F. This environmentally friendly epoxy displays excellent chemical resistance, water insensitivity, and UV resistance. EP QS will provide a glossy smooth finish when fully cured. Aggregate can be broadcast into this self-leveling material to provide a non-skid surface. EP QS emits virtually no odors and can be applied indoors with minimal disturbance contributed to high VOC levels found in most epoxies and polyurethanes.

ApplicationsEP QS adheres well to several substrates including concrete, steel, and wood. Some typical uses include:

  • CHEMICAL RESISTANT SECONDARY CONTAINMENT
  • OFFSHORE PLATFORMS
  • MAINTENANCE FACILITIES
  • PRIMER FOR MOST POLYUREAS/POLYURETHANES
  • USDA AND FDA ACCEPTABLE COATING
  • INDUSTRIAL FLOORING
  • TANK COATING
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Viscosity 100 cP100 cPHardener
     1500 cP1500 cPResin
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore D 7070ASTM D2240
    Tensile Strength 61.23 MPa8881 psiASTM D638
    Elongation at Break 28 %28 %ASTM D638
    Flexural Strength 87.370 MPa12672 psiASTM D790
    Flexural Modulus 3.34 GPa485 ksiASTM D638
    Adhesive Bond Strength 1.72 MPa250 psiWood (no primer), Delamination; ASTM D4541 Elcometer
     >= 2.07 MPa>= 300 psiConcrete (no primer), Concrete Failure; ASTM D4541 Elcometer
     >= 10.3 MPa>= 1500 psiSteel (no primer), Substrate Failure; ASTM D4541 Elcometer
    Izod Impact, Notched 3.74 J/cm7.00 ft-lb/inASTM D628
    Taber Abrasion, mg/1000 Cycles 8080CS17 Wheel, 1kg; ASTM D4060
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C145 °FASTM D648
    Flash Point >= 93.3 °C>= 200 °FASTM Pensky-Martin
     
    Processing PropertiesMetricEnglishComments
    Tack-Free Time >= 150 min
    @Temperature 75.0 °C
    >= 2.50 hour
    @Temperature 167 °F
    Gel Time 20.0 min20.0 min75°C
     
    Compliance PropertiesMetricEnglishComments
    USDA YesYes
     
    Descriptive Properties
    ColorLight Gray, Dark Gray
    Resistance to Acetic Acid (100%)Recommended
    Resistance to AcetoneRecommended
    Resistance to Ammonium Hydroxide (50%)Recommended
    Resistance to Brake Fluid (310g/l)Recommended
    Resistance to Brine-Saturated H2ORecommended Resistance to Brine-Saturated H2O (310g/l)
    Resistance to GasolineRecommended
    Resistance to H2ORecommended
    Resistance to Hydrochloric Acid (50%)Recommended
    Resistance to MEKRecommended
    Resistance to MethanolRecommended
    Resistance to Muriatic Acid (10%)Recommended
    Resistance to NaCl/H2O (10%)Recommended
    Resistance to Nitric Acid (20%)Recommended Conditional
    Resistance to Potassium Hydroxide (10%)Recommended
    Resistance to Potassium Hydroxide (20%)Recommended, Discoloration
    Resistance to Sodium BicarbonateRecommended
    Resistance to Sodium Hydroxide (50%)Recommended, Discoloration
    Resistance to Sodium Hypochlorite (10%)Recommended
    Resistance to Sugar/H2ORecommended
    Resistance to Sulfuric Acid (>50%)Recommended
    Resistance to Sulfuric Acid (10%)Recommended
    Resistance to Xylene Recommended Conditional

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Abatron AboCast 7703-21/AboCure 7703-23 (C) Epoxy Adhesive and Casting Compound
    A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
    DSM Somos® ProtoGen™ 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2
    Malvern Minerals Trikup® PT Silane Treated Aluminum Hydroxide
    Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled

    PACC082 / 22209

    Metal adhesives

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.