MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe DuraTech™ M4 Powder Metal High Speed Steel (ASTM M4)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large volume of vanadium carbides provides the high wear resistance. The high impact toughness and high transverse bend strength are results of the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure. DuraTech M4 offers improved cutting tool life compared to conventionally-wrought M1, M2, M7, and other lower-alloyed high speed steels. DuraTech M4 also excels in cold work tooling applications, where it provides better toughness and wear resistance than high-carbon, high-chromium die steels such as D2 and D3.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.92 g/cc7.92 g/cc
Density 7.92 g/cc0.286 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 5757538°C Test Temperature; Oil Quenched from 1204°C; 552°C Triple Temper Temperature
 65.565.522°C Test Temperature; Oil Quenched from 1204°C; 552°C Triple Temper Temperature
 20
@Temperature 704 °C
20
@Temperature 1300 °F
Oil Quenched from 1204°C; 552°C Triple Temper Temperature
Modulus of Elasticity 214 GPa31000 ksi
Machinability 40 - 45 %40 - 45 %1% Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.53 µm/m-°C
@Temperature 38.0 - 260 °C
5.29 µin/in-°F
@Temperature 100 - 500 °F
 12.24 µm/m-°C
@Temperature 38.0 - 649 °C
6.800 µin/in-°F
@Temperature 100 - 1200 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 840 °C1540 °FCritical Temperaure Ac1
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.45 %1.45 %
Chromium, Cr 4.5 %4.5 %
Iron, Fe 79 %79 %
Manganese, Mn 0.25 %0.25 %
Molybdenum, Mo 5.2 %5.2 %
Silicon, Si 0.25 %0.25 %
Tungsten, W 5.5 %5.5 %
Vanadium, V 3.85 %3.85 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M4 Molybdenum High Speed Tool Steel (UNS T11304)
Plywood
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel
Crucible Steel REX® M4 High Speed Steel
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel

NTIMK075 / 19422

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.