MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm Plexiglas® XT 0A000 (20070) Extruded Acrylic  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: Description: PLEXIGLAS® XT extruded acrylic has the following properties:
  • absolutely colorless and clear
  • break-resistant to impact-resistant (PLEXIGLAS RESIST®)
  • unequalled resistance to weathering and ageing
  • very good surface; brilliant, textured or satin (PLEXIGLAS SATINICE®)
  • sheets, tubes, round rods, multi-skin sheets, corrugated sheets, mirror sheets
  • 1.5 to 25 mm solid sheet thickness, multi-skin sheets 16 mm and 32 mm thick
  • standard size up to 4050 x 2050 mm (+ extra lengths)
  • more than 25 standard colors
  • good resistance to dilute acids
  • limited resistance to organic solvents
  • good resistance to alkalis
  • easy to work, similar to hardwood
  • easy to thermoform under optimal constant conditions
  • easily bonded also with solvent adhesives (e.g. ACRIFIX® 116, 117)
  • burns more or less like hardwood; very little smoke generation
  • max. service temperature approx. 70 °C

Specific Notes for this Material: Standard grade for solid sheets; largely UV-absorbing.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Water Absorption 0.44 %0.44 %24 hrs, 23°C from dry state; ISO 62, Method 1
Water Absorption at Saturation 2.1 %2.1 %Max. Weight Gain During Immersion; ISO 62, Method 1
Moisture Expansion 0.50 %0.50 %Possible Expansion due to heat and moisture
Moisture Vapor Transmission 55.0 cc-mm/m²-24hr-atm140 cc-mil/100 in²-24hr-atm
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 175 MPa25400 psiH961/30; ISO 2039-1
Tensile Strength at Break 72.0 MPa10400 psiISO 527-2/1B/5
 100 MPa
@Temperature -40.0 °C
14500 psi
@Temperature -40.0 °F
ISO 527-2/1B/5
Tensile Strength, Ultimate 35.0 MPa
@Temperature 70.0 °C
5080 psi
@Temperature 158 °F
ISO 527-2/1B/5
Elongation at Break 4.5 %4.5 %ISO 527-2 1B/5
Modulus of Elasticity 3.30 GPa479 ksiShort Time Value; ISO 527-2/1B/1
Flexural Strength 105 MPa15200 psi5 mm/min (80x10x4 mm); ISO 178
Compressive Yield Strength 103 MPa14900 psiISO 604
Poissons Ratio 0.37
@Temperature 23.0 °C
0.37
@Temperature 73.4 °F
dilation speed of 5% per min; up to 2% dilation; ISO 527-1
Shear Modulus 1.70 GPa247 ksiDynamic Shear Modulus at 10 Hz; ISO 537
Izod Impact, Notched (ISO) 1.60 kJ/m²0.761 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 1.50 J/cm²7.14 ft-lb/in²ISO 179/1fU
Impact 1212mm, Resistance to puck impact from thickness, Test Certificate No. From FMPA Stuttgart - 46/900 550; Similar to DIN 18032, part 3
Coefficient of Friction 0.450.45steel/plastic
 0.500.50plastic/steel
 0.800.80plastic/plastic
Abrasion 20 - 3020 - 30% Haze, Abrasion resistance in Taber abrader test (100 rev.;5.4 N; CS-10F); ISO 9352
Sound Insulation 26 dB26 dBWeighted Sound Reduction Index at 4 mm
 30 dB30 dBWeighted Sound Reduction Index at 6 mm
 32 dB32 dBWeighted Sound Reduction Index at 10 mm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDIN VDE 0303, Part 3
Surface Resistance 5.00e+13 ohm5.00e+13 ohmDIN VDE 0303, Part 3
Dielectric Constant  2.8
@Frequency 100000 Hz
2.8
@Frequency 100000 Hz
DIN VDE 0303, Part 4
 3.7
@Frequency 50 Hz
3.7
@Frequency 50 Hz
DIN VDE 0303, Part 4
Dielectric Strength 30.0 kV/mm762 kV/inDIN VDE 0303, Part 2
Dissipation Factor  0.030
@Frequency 100000 Hz
0.030
@Frequency 100000 Hz
DIN VDE 0303, Part 4
 0.060
@Frequency 50 Hz
0.060
@Frequency 50 Hz
DIN VDE 0303, Part 4
Comparative Tracking Index 600 V600 VDIN VDE 0303, Part 1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 0.000 - 50.0 °C
38.9 µin/in-°F
@Temperature 32.0 - 122 °F
DIN 53752A
Specific Heat Capacity 1.47 J/g-°C0.351 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°FDIN 52612
Maximum Service Temperature, Air 70.0 °C158 °FPermanent
 180 °C356 °FIR Radiator
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75
Vicat Softening Point 103 °C217 °FISO 306, Method B 50
Flash Point 430 °C806 °FIgnition Temperature; DIN 51794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491
@Thickness 3.00 mm
1.491
@Thickness 0.118 in
clear grade; ISO 489
Transmission, Visible 92 %
@Thickness 3.00 mm
92 %
@Thickness 0.118 in
clear grade; DIN 5036, Part 3
UV Transmittance 0.00 %
@Thickness 3.00 mm
0.00 %
@Thickness 0.118 in
clear grade
Reflection Coefficient, Visible (0-1) 0.040
@Thickness 3.00 mm
0.040
@Thickness 0.118 in
clear grade, Reflection loss in the visible range (for each surface)
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= 80.0 °C>= 176 °FReverse Forming Temperature
 150 - 160 °C302 - 320 °FForming Temperature
 
Descriptive Properties
Adsorption in the Visible RangeMax 0.05%clear grade, 3 mm
Fire RatingB 2, Normally FlammableDIN 4102
 Class 3BS 476 Part 7 + 6
 M 4NF P 92 501 + 92 505
 TP(b)BS 2782, Method 508A
Min Cold Bending Radius330 x thickness
Permeability to Air8.3x10-15 g cm/cm2 h Pa
Permeability to CO21.1x10-13 g cm/cm2 h Pa
Permeability to N24.5x10-15 g cm/cm2 h Pa
Permeability to O22x10-14 g cm/cm2 h Pa
Sound Velocity2700-2800 m/sat room temperature
Total Energy Transmittance g85%clear grade, 3 mm, DIN EN 410
U Value for 10mm4.4 W/m2KDIN 4701
U Value for 1mm5.8 W/m2KDIN 4701
U Value for 3mm5.6 W/m2KDIN 4701
U Value for 5mm5.3 W/m2KDIN 4701

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röhm Plexiglas® XT 0A070 (29070) Extruded Acrylic
Röhm Plexiglas® XT Soundstop® Extruded Acrylic
Röhm Plexiglas® GS 0F00 (222) Cast Acrylic
Overview of materials for Acrylic, Extruded
Röhm ACRYLITE® Extruded Acrylic Sheet

PHUK046 / 47180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.