MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Material Notes:

Applications
The PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.

Regulatory Status
The LP 5002 base resin meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
Specific recommendations for processing LP 5002 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.946 g/cc0.0342 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourF50; ASTM D1693
ESCR, Bottle >= 1000 hour>= 1000 hourF50; ASTM D2561
Melt Flow 0.20 g/10 min0.20 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Yield 23.4 MPa3400 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 0.965 GPa140 ksiASTM D790
Tensile Impact 131 J/cm245 ft-lb/inASTM D1822
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C151 °FASTM D648
Vicat Softening Point 122 °C252 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
AntistatNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM 5502-01 Polyethylene, Sheet/Thermoforming Grade, HDPE
Chevron Phillips Marlex® HHM 5202 Polyethylene, Sheet/Thermoforming Grade, HDPE
Chevron Phillips Marlex® HHM 5502LW Polyethylene; HDPE
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE
LyondellBasell Petrothene® LR732013 High Density Polyethylene (Blow Molding Grade)

PEQU0166 / 36595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.