MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: General Notes on Meldin 3000/5000 Series Bearing Products:
Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.
Specific Notes on Meldin® 5055 Bearing
Meldin® 5055 low-friction, wear resistant bearings custom molded from Meldin® 5055 compound perform at high loads and high temperatures with minimal deformation. Meldin® 5055 is self-lubricating, operates quietly, and is resistant to most chemicals and fluids.
Information provided by Saint Gobain Performance Plastics.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Water Absorption 0.20 %0.20 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 112 MPa16200 psiASTM D638
Elongation at Break 1.2 %1.2 %ASTM D638
Elongation at Yield 1.2 %1.2 %ASTM D638
Tensile Modulus 15.9 GPa2310 ksiASTM D 638
Flexural Strength  14.5 MPa
@Temperature 288 °C
2100 psi
@Temperature 550 °F
ASTM D790
 182 MPa
@Temperature 23.0 °C
26400 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus  0.860 GPa
@Temperature 288 °C
125 ksi
@Temperature 550 °F
ASTM D790
 14.5 GPa
@Temperature 23.0 °C
2100 ksi
@Temperature 73.4 °F
ASTM D790
Compressive Strength 124 MPa18000 psiASTM D695
Compressive Modulus 3.10 GPa450 ksiASTM D695
Poissons Ratio 0.420.42
Coefficient of Friction, Dynamic 0.20 - 0.230.20 - 0.23Dry; ASTM D3702
 
Thermal PropertiesMetricEnglishComments
CTE, linear  41.0 µm/m-°C
@Temperature 24.0 - 143 °C
22.8 µin/in-°F
@Temperature 75.2 - 289 °F
Below Tg; ASTM E831
 50.0 µm/m-°C
@Temperature >=143 °C
27.8 µin/in-°F
@Temperature >=289 °F
Above Tg; ASTM E831
Thermal Conductivity 0.760 W/m-K5.27 BTU-in/hr-ft²-°FASTM F433
Melting Point 343 °C649 °FASTM D3418
Maximum Service Temperature, Air 316 °C600 °FUL-746 B
Deflection Temperature at 1.8 MPa (264 psi) 316 °C601 °FASTM D648
Glass Transition Temp, Tg 143 °C289 °FASTM D3418
 
Descriptive Properties
Hardness, Rockwell K24.9ASTM D785

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
DuPont Mobility and Materials Vespel® SCP-5009 Polyimide
Saint-Gobain Meldin® 5320 Thermoplastic Bearing Material
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material
Saint-Gobain Meldin® 5015 Bearing

PSTGQZ112 / 68624

Ensinger SPI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.