MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI Type 651 (19-9 DL) Stainless Steel
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 600 Series Stainless Steel

Material Notes: 60 mm diameter bar, warm rolled and stress relieved at 730°C for 8 hours with hardness of 220-241 HB

Key Words: UNS K63198, AMS 5369, AMS 5526, AMS 5527, AMS 5720, AMS 5721, AMS 5722, ASTM A453, ASTM A457, ASTM 458, ASTM A477, SAE J467(19-9 DL), MIL SPEC MIL-S-46042
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.94 g/cc0.287 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 838 MPa122000 psi
 331 MPa
@Temperature 815 °C
48000 psi
@Temperature 1500 °F
 365 MPa
@Temperature 760 °C
52900 psi
@Temperature 1400 °F
 459 MPa
@Temperature 705 °C
66600 psi
@Temperature 1300 °F
 534 MPa
@Temperature 650 °C
77500 psi
@Temperature 1200 °F
 614 MPa
@Temperature 540 °C
89100 psi
@Temperature 1000 °F
 634 MPa
@Temperature 480 °C
92000 psi
@Temperature 896 °F
 672 MPa
@Temperature 370 °C
97500 psi
@Temperature 698 °F
 703 MPa
@Temperature 150 °C
102000 psi
@Temperature 302 °F
 707 MPa
@Temperature 260 °C
103000 psi
@Temperature 500 °F
Tensile Strength, Yield 579 MPa
@Strain 0.2 %
84000 psi
@Strain 0.2 %
 279 MPa
@Strain 0.2 %,
Temperature 815 °C
40500 psi
@Strain 0.2 %,
Temperature 1500 °F
 317 MPa
@Strain 0.2 %,
Temperature 760 °C
46000 psi
@Strain 0.2 %,
Temperature 1400 °F
 352 MPa
@Strain 0.2 %,
Temperature 705 °C
51100 psi
@Strain 0.2 %,
Temperature 1300 °F
 362 MPa
@Strain 0.2 %,
Temperature 650 °C
52500 psi
@Strain 0.2 %,
Temperature 1200 °F
 396 MPa
@Strain 0.2 %,
Temperature 540 °C
57400 psi
@Strain 0.2 %,
Temperature 1000 °F
 427 MPa
@Strain 0.2 %,
Temperature 480 °C
61900 psi
@Strain 0.2 %,
Temperature 896 °F
 455 MPa
@Strain 0.2 %,
Temperature 370 °C
66000 psi
@Strain 0.2 %,
Temperature 698 °F
 496 MPa
@Strain 0.2 %,
Temperature 260 °C
71900 psi
@Strain 0.2 %,
Temperature 500 °F
 517 MPa
@Strain 0.2 %,
Temperature 150 °C
75000 psi
@Strain 0.2 %,
Temperature 302 °F
Elongation at Break 43 %43 %in 50 mm
 20.5 %
@Temperature 760 °C
20.5 %
@Temperature 1400 °F
in 50 mm
 27.5 %
@Temperature 260 °C
27.5 %
@Temperature 500 °F
in 50 mm
 29 %
@Temperature 815 °C
29 %
@Temperature 1500 °F
in 50 mm
 29 %
@Temperature 705 °C
29 %
@Temperature 1300 °F
in 50 mm
 29.5 %
@Temperature 480 °C
29.5 %
@Temperature 896 °F
in 50 mm
 29.5 %
@Temperature 540 °C
29.5 %
@Temperature 1000 °F
in 50 mm
 30 %
@Temperature 150 °C
30 %
@Temperature 302 °F
in 50 mm
 30.5 %
@Temperature 650 °C
30.5 %
@Temperature 1200 °F
in 50 mm
 31.5 %
@Temperature 370 °C
31.5 %
@Temperature 698 °F
in 50 mm
Reduction of Area 55.5 %55.5 %
 46 %
@Temperature 540 °C
46 %
@Temperature 1000 °F
 47.5 %
@Temperature 650 °C
47.5 %
@Temperature 1200 °F
 48.5 %
@Temperature 480 °C
48.5 %
@Temperature 896 °F
 49 %
@Temperature 705 °C
49 %
@Temperature 1300 °F
 49.5 %
@Temperature 260 °C
49.5 %
@Temperature 500 °F
 49.5 %
@Temperature 370 °C
49.5 %
@Temperature 698 °F
 52.5 %
@Temperature 150 °C
52.5 %
@Temperature 302 °F
 56.5 %
@Temperature 760 °C
56.5 %
@Temperature 1400 °F
 62 %
@Temperature 815 °C
62 %
@Temperature 1500 °F
Modulus of Elasticity 200 GPa29000 ksiTypical for stainless steel
Machinability 45 %45 %Based on 100% machinability for AISI 1212 steel.
Charpy Impact 62.0 J45.7 ft-lbV-Notch; Hot-Rolled/Stress Relieved at 650°C.
 
Thermal PropertiesMetricEnglishComments
CTE, linear  15.3 µm/m-°C
@Temperature 21.0 - 93.0 °C
8.50 µin/in-°F
@Temperature 69.8 - 199 °F
 16.3 µm/m-°C
@Temperature 21.0 - 205 °C
9.06 µin/in-°F
@Temperature 69.8 - 401 °F
 16.7 µm/m-°C
@Temperature 21.0 - 315 °C
9.28 µin/in-°F
@Temperature 69.8 - 599 °F
 17.6 µm/m-°C
@Temperature 21.0 - 540 °C
9.78 µin/in-°F
@Temperature 69.8 - 1000 °F
 18.0 µm/m-°C
@Temperature 21.0 - 815 °C
10.0 µin/in-°F
@Temperature 69.8 - 1500 °F
Specific Heat Capacity 0.420 J/g-°C
@Temperature 0.000 - 100 °C
0.100 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity 13.5 W/m-K93.7 BTU-in/hr-ft²-°F
 18.5 W/m-K
@Temperature 425 °C
128 BTU-in/hr-ft²-°F
@Temperature 797 °F
 21.3 W/m-K
@Temperature 650 °C
148 BTU-in/hr-ft²-°F
@Temperature 1200 °F
Melting Point 1420 - 1435 °C2590 - 2615 °F
Solidus 1420 °C2590 °F
Liquidus 1435 °C2615 °F
Maximum Service Temperature, Air 780 °C1440 °FContinuous Service
 955 °C1750 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.28 - 0.35 %0.28 - 0.35 %
Chromium, Cr 18 - 21 %18 - 21 %
Copper, Cu <= 0.50 %<= 0.50 %
Iron, Fe 64 %64 %
Manganese, Mn 0.75 - 1.5 %0.75 - 1.5 %
Molybdenum, Mo 1.0 - 1.75 %1.0 - 1.75 %
Nickel, Ni 8.0 - 11 %8.0 - 11 %
Niobium, Nb (Columbium, Cb) 0.25 - 0.60 %0.25 - 0.60 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.30 - 0.80 %0.30 - 0.80 %
Sulfur, S <= 0.030 %<= 0.030 %
Titanium, Ti 0.10 - 0.35 %0.10 - 0.35 %
Tungsten, W 1.0 - 1.75 %1.0 - 1.75 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for T 600 Series Stainless Steel
661 Stainless Steel
329 Stainless Steel, annealed bar
17-7 PH Stainless Steel, CH900, wire
Overview of materials for T 300 Series Stainless Steel

MQ651A / 13223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.