MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® 607 Nylon 6, Extrusion Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Dry as molded. Extrusion grade. Nylene 607 is a very high viscosity extrusion resin having an ASTM relative viscosity of 800. Nylene 607 has excellent structural strength, durability, and physical properties. It has good melt strength and good draw-down properties which promote dimensional control for extrusion of pipe, tubing, film, and sheet. It is particularly recommended for the extrusion of thick slab, large rod stock, and large complex profiles. Optimum processing conditions should permit for a melt temperature of 550 - 575ºF at the die.

ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 0.020 %0.020 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psiASTM D638
Elongation at Break 210 %210 %ASTM D638
Flexural Yield Strength 107 MPa15500 psiASTM D790
Izod Impact, Notched 0.400 J/cm0.749 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 186 °C367 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 295 °C563 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nylene® NX4301 Nylon 6, Extrusion Grade
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Nurel Engineering Polymers Promyde® B40 L PA 6, Dry, Lubricated
LyondellBasell Alathon 8005M-3 High Denisty Polyethylene

PN6C54 / 54238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.