MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Micropol Microlink XL28/FR Black Crosslinkable Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Flame retardant. Provides a finished molding of improved properties with the use of conventional rotational molding equipment. Properties include enhanced toughness (particularly low temp impact), ESCR, chemical, and temperature resistance. It is fully UV stabilized and available in colors for outdoor use in all climates; minimum UV10 rating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour>= 1000 hourM F50; ASTM D1693
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 23.0 MPa3340 psi50mm/min; ASTM D638
Elongation at Break 350 %350 %ASTM D638
Flexural Modulus 0.750 GPa109 ksiASTM D790
Impact 36
@Temperature -20.0 °C
36
@Temperature -4.00 °F
J/mm, Micropol test based on ASTM D1790
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -120 °C<= -184 °FASTM D746
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Multibase Multi-Flam™ 0107 HDPE Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable
Micropol Microlink XL28 Crosslinkable Polyethylene
Micropol Isoplas P651 Crosslinkable Polyethylene
Micropol Isoplas P381 Crosslinkable Polyethylene

PMICRO27 / 108457

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.