MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PSC 1340 Crystal Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Transparent Grade

Material Notes: 1340 is a high molecular weight crystal polystyrene which allows maximum dilution rates with high impact polystyrene grades such as LACQRENE® 7240. In dilution, LACQRENE® 1340 gives excellent processing in both extrusion and thermoforming with good finished product dimensional stability.

Application

Cups and other products by in line extrusion/thermoforming, Foamed trays by direct gassing (in line thermoforming), Shower screens

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines. This product was previously known as LACQRENE®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Water Absorption <= 0.10 %<= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/in
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 7070ISO 2039-2
Tensile Strength at Break 44.0 MPa6380 psiISO 527-2
Elongation at Break 2.5 %2.5 %ISO 527-2
Tensile Modulus 3.10 GPa450 ksiISO 527-2
Flexural Modulus 2.90 GPa421 ksiISO 178
Charpy Impact Unnotched 0.800 J/cm²3.81 ft-lb/in²ISO 179/1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+14 ohm>= 1.00e+14 ohmISO IEC93
Dielectric Strength 135 kV/mm3430 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 71.0 µm/m-°C
@Temperature 20.0 °C
39.4 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FAnnealed; ISO 75-2B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FUnannealed; ISO 75-2A
Vicat Softening Point 93.0 °C199 °F50N (T° increase = 5°C/h); ISO 306B50
 98.0 °C208 °F10N (T° increase = 50°C/h); ISO 306A50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSC 1540(AS) Crystal Polystyrene
Total PSC 1540(EU) Crystal Polystyrene
Total PSC 1960N Crystal Polystyrene
Total PSC 1160/1160N Crystal Polystyrene
Total PSC 1810/1811 Polystyrene

PFINAA025 / 38461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.