MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik Vestamid® L1600 nf (dry properties) Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes:

ISO data as provided by the manufacturer.

Key Words: Polyamide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³
Water Absorption 1.0 %1.0 %
Moisture Absorption at Equilibrium <= 0.50 %<= 0.50 %Humidity Absorption
Melt Flow 100 g/10 min100 g/10 min
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psi
Elongation at Break >= 50 %>= 50 %
Elongation at Yield 5.0 %5.0 %
Modulus of Elasticity 1.40 GPa203 ksi
Charpy Impact Unnotched NBNB
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Tensile Creep Modulus, 1 hour 800 MPa116000 psi
Tensile Creep Modulus, 1000 hours 500 MPa72500 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  2.0
@Frequency 1e+6 Hz
2.0
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dielectric Strength 26.0 kV/mm660 kV/in
Dissipation Factor  0.028
@Frequency 1e+6 Hz
0.028
@Frequency 1e+6 Hz
 0.041
@Frequency 100 Hz
0.041
@Frequency 100 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow <= 50.0 µm/m-°C
@Temperature 20.0 °C
<= 27.8 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 120 °C248 °F
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °F
Vicat Softening Point 140 °C284 °F50°C/hr/50 N
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM)
Overview of materials for Acetal Homopolymer, Unreinforced
Overview of materials for Nylon 6, Extruded
Evonik Vestamid® L2101F Nylon 12
Evonik Vestamid® LX9007 Nylon 12

PHUL44 / 47304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.