MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek RB B4C Reaction-Bonded Boron Carbide
Categories: Ceramic; Carbide

Material Notes: Low density for ultra-lightweight designs

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.65 g/cc0.0957 lb/in³ASTM-C 20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 25.525.5Gpa; KNOOP 1000 gm
Modulus of Elasticity 379 GPa55000 ksiASTM-C848
Flexural Strength 250 MPa36300 psiMOR; ASTM-F417
Compressive Strength 1721 MPa249600 psiASTM-C773
Poissons Ratio 0.180.18ASTM-C848
Fracture Toughness 3.00 - 4.00 MPa-m½2.73 - 3.64 ksi-in½KIC; Notched Beam
Shear Modulus 161 GPa23400 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.50 µm/m-°C
@Temperature 25.0 - 1000 °C
2.50 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM-C372
Thermal Conductivity 50.0 W/m-K347 BTU-in/hr-ft²-°FASTM-C408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Boron Carbide, B4C
Ceradyne Ceralloy® 546 Boron Carbide
Goodfellow Hot Pressed Boron Carbide B4C
Ceradyne Ceralloy® 546-3E Boron Carbide
American Elements Boron Carbide Nanoparticles

CCOOR914 / 104618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.