MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Purell PE1840H Low Density Polyethylene, Blown Film, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Blow Molding Grade

Material Notes: Purell PE 1840 H is a low density polyethylene with good flexibility and is delivered in pellet form. It is designed for small blow molding but can also be used in film applications and injection molding. It can be used for medical devices and packaging of pharmaceuticals.

Regulatory Status: Purell PE 1840 H meets the requirements of the Food and Drug Administration, Code of Federal Regulations, 21CFR Section 177.1520. This regulation allows the use of this olefin polymer in "articles or components of articles intended for use in contact with food."

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D1505
Thickness 50.8 microns2.00 mil
Melt Flow 1.5 g/10 min1.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4747ASTM D2240
Tensile Strength at Break 12.2 MPa1770 psiASTM D638
Tensile Strength, Yield 10.8 MPa1560 psiASTM D638
Elongation at Break 670 %670 %ASTM D638
Tensile Modulus 0.254 GPa36.9 ksi1% Secant; ASTM D638
Flexural Modulus, 1% Secant 241 MPa35000 psiASTM D790
Dart Drop 2.36 g/micron60.0 g/milASTM D1709
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 87.0 °C189 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze <= 11 %<= 11 %ASTM D1003
Gloss >= 20 %>= 20 %20°; ASTM D2457
 75 %75 %Gardner, 60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 °C356 °F
Blow-up Ratio (BUR) 2.02.0
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Purell PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
LyondellBasell Petrothene® NA247000 Low Density Polyethylene, Injection Molding Grade
LyondellBasell Purell PE3220D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
A. Schulman CP763-01 Extruded, Blow Molding and Injection Molding Grade Polyethylene
LyondellBasell Lupolen 2420 F LDPE

PEQU0833 / 104189

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.