MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Available in standard black.

Information provided by MBA Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³MBA Method
Melt Flow 5.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 20.0 MPa
@Temperature 23.0 °C
2900 psi
@Temperature 73.4 °F
ISO 527-2/50
Flexural Modulus 1.00 GPa
@Temperature 23.0 °C
145 ksi
@Temperature 73.4 °F
ISO 178
Izod Impact, Notched (ISO)  6.00 kJ/m²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 51.0 °C124 °Funannealed; ISO 75-1A
Vicat Softening Point 60.0 °C140 °FVST/B/50; ISO 306
 135 °C275 °FVST/A/50; ISO 306
Glow Wire Flammability Index 650 °C
@Thickness 2.00 mm
1200 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 210 °C356 - 410 °FExtrusion Range
 200 °C392 °FRecommended Extrusion
 200 °C392 °FRecommended Injection Molding
 190 - 220 °C374 - 428 °FInjection Molding Range
Mold Temperature 40.0 °C104 °FRecommended
 30.0 - 60.0 °C86.0 - 140 °F
Drying Temperature 80.0 °C
@Time 3600 - 7200 sec
176 °F
@Time 1.00 - 2.00 hour
Moisture Content <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unipetrol PP MONSTEN® MB 720 Polypropylene Impact Copolymer
Unipetrol PP MONSTEN® MA 611 Polypropylene Impact Copolymer
Unipetrol PP MONSTEN® MA 712 Polypropylene Impact Copolymer
Unipetrol PP MONSTEN® MA 745 Polypropylene Impact Copolymer
Unipetrol PP MONSTEN® MA 612 Polypropylene Impact Copolymer

PMBAP994 / 161701

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.