MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polimersan Plastics POLIKES® (PA 6 G) Cast Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Cast

Material Notes: POLIKES® PA6 G (CAST POLYAMIDE) is a plastic with high physical, electrical and chemical resistance. Its resistance is high especially against strokes and loads. Its temperature resistance is high, whereas corrosion coefficient is low. But, because of its water absorption property, it is not recommended at humid environments(%6-7).

PROPERTIES OF POLIKES®:

  • 100°C Service Temperature
  • Low Corrosion Coefficient
  • Very High Pressing Resistance
  • High Hardness
  • High Resistance To Strokes
  • Resistance To Heat
  • Resistance To Chemical Substances
  • Lower Water Absorption compared to PA 6
GENERAL USAGE AREAS OF POLIKES®:
  • Sledges
  • Wheels
  • Rolls
  • Gears
  • Bearings
  • Bobbins
  • Hoops
  • Corrosion Plates
  • Food Industry Parts
  • Chemical Industry Parts
  • Paper Industry Parts
  • Textile Industry Parts
  • Press Industry Parts

Information provided by Polimersan Polimer Kimya San.Tic.Ltd.Sti.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO.1183 DN.53479
Water Absorption 6.0 - 7.0 %6.0 - 7.0 %ISO.62 DN.53495
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8888ISO.2039-2
Hardness, Shore D 8585DN.53505
Ball Indentation Hardness 110 - 160 MPa16000 - 23200 psiISO.2039-2
Tensile Strength at Break 88.0 - 90.0 MPa12800 - 13100 psiISO.527 DN.53455
Tensile Strength, Yield 55.0 - 85.0 MPa7980 - 12300 psiISO.527 DN.53455
Elongation at Break 10 - 40 %10 - 40 %ISO.527 DN.53455
Modulus of Elasticity 3.90 - 4.20 GPa566 - 609 ksiISO.178 DN.53452
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmISO.167 DN.53482
Surface Resistance >= 1.00e+12 ohm>= 1.00e+12 ohmISO.167 DN.53482
Dielectric Strength 80.0 - 100 kV/mm2030 - 2540 kV/inISO.243 DN.53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 - 90.0 µm/m-°C
@Temperature 20.0 °C
44.4 - 50.0 µin/in-°F
@Temperature 68.0 °F
DN.53752
Melting Point 190 °C374 °F
Maximum Service Temperature, Air 100 °C212 °FISO.75 DN.53461

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polikim KESTAMID® PA6G Polyamide 6
GEHR Plastics PA 6 G Nylon 6, Cast, Dry
Omnia Plastica Omniamid PA 6 - Akulon 6 - Dry
Overview of materials for Nylon 6, Unreinforced
Polikim KESTAMID® HS Polyamide 6, Heat Resistant

PPOLIM05 / 56971

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.